1. Why are the overlaps of galvanized color-coated steel coils a major risk point for leakage?
A: The overlap is not a completely continuous whole and has the following inherent weaknesses:
Gap: Even when two sheets are pressed tightly together, capillary gaps remain, allowing rainwater to seep in due to siphon effect;
Thermal expansion and contraction: The expansion and contraction of the color-coated steel sheets under temperature differences can cause relative displacement at the overlap, compromising the seal;
Mechanical stress: Foot traffic, wind loads, or vibrations can loosen or deform the overlap;
Cutting corrosion: If the cut edges of the overlap are not rust-proofed, the expansion of rust will widen the gaps, further exacerbating leakage.
Therefore, simply relying on overlapping is insufficient for reliable waterproofing; specialized sealing measures must be taken.

2. What is the most common and reliable method for waterproofing overlapping galvanized color-coated steel coils?
A: The "sealant sealing + mechanical fixing" combination method consists of three steps:
Applying special sealant: Continuously apply neutral silicone weather-resistant sealant or butyl tape between the overlapping surfaces (or at the edge of the overlapping seam) to form an elastic waterproof layer;
Proper fixing: Fix the overlapping area with self-tapping screws or rivets at certain intervals (usually ≤200mm) to ensure a tight fit between the two plates and prevent the sealant layer from cracking;
Edge finishing: Create a drip line or apply sealant at the end of the overlap (the lower plate end in the direction of water flow) to prevent water from flowing back along the seam.
For temporary structures or indoor environments with less stringent requirements, double-sided butyl tape can also be used for pressing, but the long-term reliability is not as good as using screws.

3. What are the advantages and disadvantages of sealant and butyl tape? How to choose?
A:Material | Advantages | Disadvantages | Applicable Scenarios
Neutral Silicone Weatherproof Sealant | Good elasticity, aging resistance, strong adhesion, can be brushed for repair | Requires curing time (generally 24 hours to cure), requires caulking gun during construction, high surface cleanliness requirements | Permanent buildings, roofs, long-term waterproofing of walls
Butyl Tape | Extremely fast construction (peel and apply), instant sealing, no curing required, excellent water and air tightness | Not resistant to long-term direct UV radiation (must be covered), weak tensile and shear strength, may flow at high temperatures | Internal sealing of overlaps covered by upper panels, temporary buildings, emergency repairs

4. What are the specific requirements for overlap width and panel type in waterproofing?
A: The minimum overlap width to meet waterproofing requirements depends on the panel type, slope, and load:
Roof (slope ≥ 5%):
Corrugated panels: ≥ one complete wave pitch (usually ≥ 150mm);
Trapezoidal panels: ≥ 120mm (≥ 200mm without sealant);
With sealant, it can be appropriately reduced to 80-100mm, but not less than 50mm.
Walls: Usually ≥ 100mm, and the upper panel should cover the outer side of the lower panel (overlap with water flow).
Key principle:
The overlap area must be located on purlins or supporting members and cannot be suspended.
5. If the overlap is leaking, how can it be effectively repaired without removing the panel?
A: Depending on the location and severity of the leak, choose a repair method that does not require removing the panel:
Leakage Type Repair Method (No Panel Removal Required)
Small Cracks (Efflorescence Visible When Dry)
Clean and dry, then inject a low-viscosity penetrating sealant (such as polyurea or acrylic) along the crack, or brush on liquid rubber.
Screw Holes or Localized Small Holes Leaking
Cut self-adhesive butyl tape into round or strip shapes, cover the holes, and press firmly; or apply neutral silicone sealant and smooth it with a plastic sheet.
Long Overlap Joints with Overall Leakage
First clean the crack of dust and oil → Apply quick-drying polyurethane sealant to the outer edge of the overlap joint, and embed a foam backing rod to control the thickness → Sprinkle cement or fine sand on the surface for protection (optional).