Chemical Analysis
Typical Values (Weight %)
| Nickel | 38.0 min.–46.0 max. | Iron | 22.0 min. |
| Chromium | 19.5 min.–23.5 max. | Molybdenum | 2.5 min.–3.5 max. |
| Molybdenum | 8.0 min.-10.0 max. | Copper | 1.5 min.–3.0 max. |
| Titanium | 0.6 min.–1.2 max. | Carbon | 0.05 max. |
| Niobium (plus Tantalum) | 3.15 min.-4.15 max. | Titanium | 0.40 |
| Carbon | 0.10 | Manganese | 1.00 max. |
| Sulfur | 0.03 max. | Silicon | 0.5 max. |
| Aluminium | 0.2 max. |
Mechanical Properties
Typical Room Temperature Mechanical Properties, Mill Annealed
| Yield Strength 0.2% Offset |
Ultimate Tensile Strength |
Elongation in 2 in. |
Hardness | ||
| psi (min.) | (MPa) | psi (min.) | (MPa) | % (min.) | Rockwell B |
| 49,000 | 338 | 96,000 | 662 | 45 | 135-165 |
| Temperature,°F | 70 | 400 | 600 | 800 | 1000 | 1200 | 1400 | 1600 |
| Ultimate Tensile Strength, ksi | 144 | 134 | 132 | 132 | 130 | 119 | 78 | 40 |
| 0.2% Yield Strength, ksi | 84 | 66 | 63 | 61 | 61 | 60 | 59 | 39 |
| Elongation, % | 44 | 45 | 42.5 | 45 | 48 | 34 | 59 | 117 |
Typical Rupture Strength Bar, Stress to Rupture at Indicated Time
| Temperature, °F | 1200 | 1300 | 1400 |
| 100 Hours, ksi | 59 | 34 | 18 |
| 1,000 Hours, ksi | 43 | 23 | 12 |
INCONEL and INCOLOY are registered trademarks of Special Metals (PCC)
Hot Tags: alloy 825 plates or alloy 825 nickel alloy plate, China alloy 825 plates or alloy 825 nickel alloy plate manufacturers, suppliers, factory, Galvanised Metal Steel Plate, 2mm galvanised steel sheet, galvanised steel plate 5mm, DX51D Z275 Galvanized Steel plate, 1 5mm galvanised steel sheet, steel plate galvanized