What the 0.5 x 1522 mm DC01 Coil Specification Covers
The description names four things at once: a nominal thickness of 0.5 mm, a strip width of 1522 mm, the EN 10130 grade DC01 and the delivery form of strip in coils. DC01 is the base cold forming grade of the cold rolled low carbon family and is still recorded under its older names St12 and FeP01. Because the steel is non-alloy, corrosion protection has to come from a coating, an oil film or the paint system rather than from alloying additions in the base metal.
The CRCA abbreviation on the same data sheet stands for cold reduced close annealed. It tells the buyer that the coil has been rolled cold and then annealed to soften it, instead of being delivered full hard. Skin passed adds a light temper pass of roughly 0.5 % to 1.5 % after annealing, applied to remove the sharp yield point and to set a controlled surface roughness.
Strip Width, Slitting and Coil Build
| Item | Typical range |
|---|---|
| Nominal thickness | 0.5 mm |
| Master coil width | 1522 mm, normally slit to finished widths |
| Finished slit widths | From about 20 mm upwards, depending on the slitting line |
| Coil inner diameter | 508 mm or 610 mm |
| Coil outer diameter | Up to about 1800 mm |
| Coil weight | 3 t to 15 t |
| Edge condition | Mill edge or slit edge, deburred on request |
| Delivery condition | CRCA, skin passed, lightly oiled |
Slitting a 1522 mm master coil is the normal route to saleable widths, so the slitting plan should be checked against the finished width tolerance before the order is placed: the number of cuts taken from one master coil decides both trim loss and burr height. Where the strip feeds a tube mill or a roll forming line, an agreed camber limit is more important in practice than the absolute width tolerance.
Thickness, Tolerances and Flatness
Dimensional acceptance is settled by quoting the tolerance class from EN 10131 alongside the nominal size. Thickness tolerance on cold rolled coil tightens as the gauge falls, which is why a 0.5 mm strip is far more sensitive to mill setup than a 2 mm sheet. Three checks decide whether a coil will run cleanly.
Thickness across the width. A crown or wedge profile shows up as a mismatch the moment a master coil is slit into several strips.
Width tolerance and squareness. Mill edge and slit edge are not interchangeable, so the edge condition belongs on the order.
Flatness and camber. Cross bow, edge wave and centre buckle all originate in rolling and annealing and set the practical limit on line speed.
Annealing and Skin Pass: What the Coil Has Been Through
Annealing recrystallises the work hardened structure created by cold reduction and restores ductility. The temper pass that follows is deliberately small, typically 0.5 % to 1.5 % extension, just enough to eliminate discontinuous yielding and to imprint a surface texture that carries lubricant through the die. Coil destined for painting is often ordered with a slightly rougher skin passed surface, while material for exposed bright parts is ordered smoother. Consistency matters more than the absolute value, because run to run variation in surface roughness shows up as uneven paint appearance on the finished panel.
Where 0.5 x 1522 mm Non-Alloy Strip Is Used
Longitudinal welded tube and pipe produced from slit strip
Cable armouring, strapping and banding strip
HVAC duct and ventilation components
Drum closures, ring and lid blanks
Shelving, storage and racking uprights
Perforated and expanded metal panel feedstock
Door frames, edge profiles and general sheet metal fabrication
These uses share one requirement: thickness and yield behaviour that stay the same on the first metre of coil and on the last. That is the practical reason for specifying CRCA skin passed material rather than a fully hard coil, which would need extra processing before it could be formed.
Common Questions About This Coil
Q: What does CRCA mean on a coil certificate?
Cold reduced close annealed. The strip was rolled cold to thickness and then annealed so that it is soft and ductile rather than full hard.
Q: Why does skin passing matter on 0.5 mm strip?
Thin strip forms at low force, so an unsuppressed yield point produces visible stretcher strains very easily. A light temper pass removes the yield point and steadies the flow of material in the press.
Q: Can a 1522 mm coil be supplied already slit?
Yes. Master coil is normally slit to the finished widths the customer forms, with the slitting plan agreed in advance so that trim loss and burr height stay within limits.
Q: Is DC01 a non-alloy steel?
Yes. DC01 is a low carbon non-alloy grade under EN 10130, so any corrosion resistance has to be provided by coating, oiling or painting.
Q: Which tolerance standard applies to the dimensions?
EN 10131 sets thickness, width, camber and flatness tolerances for cold rolled flat products. The required tolerance class should always be stated with the nominal size.
Q: How is the coil protected before shipment?
Coils are wrapped, eye protected and lightly oiled, then secured on saddles. Later storage indoors on a level floor or saddle keeps edge rust away from the outer wrap.