ASTM A36, Ss400, S235, S355, Q235B, Q345 HRC Gi Coil Hot Rolled Ms Mild Carbon Steel Coil Building Materials

Apr 01, 2026 Leave a message

What are the common anti-corrosion methods for S235JR?

A: Hot-dip galvanizing, epoxy zinc-rich primer, fluorocarbon topcoat, powder coating.

What is the fire resistance of S235JR?

A: Bare steel has poor fire resistance; fire-retardant coatings or fire-retardant coverings are necessary in buildings.

What is the difference between S235JR and S235J0?

A: J0 is for 0°C impact testing, while JR is for 20°C impact testing; JR is preferred for buildings operating at normal temperatures.

What is the difference between S235JR and S235J2?

A: J2 is for -20°C impact testing and is used in low-temperature environments/more critical structures.

How to choose between S235JR and S355JR?

A: S235JR is used for light-load and ordinary buildings; S355JR is used for large-span and heavy-load structures.