Minimum Cutting Sizes of Q355 Plate
The minimum cutting size depends on the cutting method and plate thickness. Flame cutting requires a minimum length and width of 100 mm; plasma cutting a minimum of 50 mm; and laser cutting a minimum of 10 mm. For smaller size requirements, fine cutting services or alternative processing methods are recommended.
Bending Q355 Plate into Arcs
Q355 plate has good plasticity and can be bent into circular arcs of various radii. The minimum bending radius is related to the plate thickness and grade: for plates up to 10 mm thick, the minimum bending radius is about 2 times the plate thickness; for plates above 10 mm, about 3 to 5 times the plate thickness. For thick plates, hot bending is recommended to prevent cracking.
Delivery States
Hot-rolled state: the most common delivery state with low cost, suitable for most structural parts. Normalized state: the plate is heated to 900 to 950 degrees C and air-cooled, giving uniform grain size, better toughness and weldability, suitable for higher performance structural parts. Tempered state: the plate is heated to a certain temperature and cooled, with lower internal stress, suitable for precision structural parts.
Thickness Tolerances
Per GB/T 3274-2017, the thickness tolerance of Q355 plate is divided into normal and precise classes. Normal tolerance: plus or minus 0.5 mm for plates up to 16 mm, plus or minus 0.8 mm for 16 to 40 mm, and plus or minus 1.0 mm above 40 mm. Precise tolerance: plus or minus 0.3 mm up to 16 mm, plus or minus 0.5 mm for 16 to 40 mm, and plus or minus 0.8 mm above 40 mm. Precise tolerance plates are available on request.
Weight Calculation Formula
The weight of a Q355 plate is calculated as weight in kg equals thickness in mm times width in meters times length in meters times density 7.85 g per cubic cm. For example, a plate 10 mm thick, 2 m wide, and 6 m long weighs 10 times 2 times 6 times 7.85, which is 942 kg.
Frequently Asked Questions
Q: What is the minimum flame cutting size?
A: Flame cutting requires a minimum length and width of 100 mm; plasma 50 mm; laser 10 mm.
Q: What is the minimum bending radius of Q355?
A: About 2 times the plate thickness for plates up to 10 mm, and 3 to 5 times for thicker plates; hot bending is recommended for thick plates.
Q: What are the common delivery states?
A> Hot-rolled, normalized, and tempered, chosen by strength, toughness, and precision requirements.
Q: What is the normal thickness tolerance of Q355?
A: Plus or minus 0.5 mm up to 16 mm, plus or minus 0.8 mm for 16-40 mm, and plus or minus 1.0 mm above 40 mm per GB/T 3274.
Q: How is plate weight calculated?
A: Thickness in mm times width in m times length in m times 7.85 g/cm3.
Q: When is normalizing required?
A> When uniform grain, better toughness, and weldability are required for higher performance structural parts.