DC01, St37 and A36 Carbon Steel Coil: Grades, Standards and Selection

Sep 08, 2025 Leave a message

Carbon steel coil is bought and sold under several designation systems at once, and the title above mixes three of them: DC01 from the European cold-rolled forming family, St37 from the German constructional steel family, and A36 from the American structural family. They are not interchangeable, and choosing the wrong one is a common cause of forming cracks, unnecessary cost or rejected deliveries. The sections below separate the three and set out the properties that actually matter when a coil is ordered.

Three Designation Families Behind One Product Name

DC01 belongs to the EN 10130 family of cold-reduced low-carbon steel for cold forming. It is a commercial-quality grade supplied as cold-rolled coil or sheet with a controlled, formable surface.

St37 belongs to DIN 17100, the older German standard for general structural steel. St37-2 was the basic grade for welded and bolted structures; its modern equivalent is S235JR under EN 10025-2.

A36 belongs to ASTM A36/A36M, the American structural carbon steel specification covering plates, shapes and bars. It is a hot-rolled structural material, not a drawing grade.

A coil can therefore be described loosely as "carbon steel coil" while behaving completely differently in the press shop, depending on which family the enquiry refers to. The first step in any quotation is to establish whether the buyer needs formability (cold-rolled family), weldability and strength (structural family), or both.

DC01 to DC04: The EN 10130 Cold Rolled Family

EN 10130 covers cold-reduced flat products with maximum limits for carbon, manganese, phosphorus and sulphur that tighten as formability increases. The headline chemistry is as follows.

Grade Formability quality C max % Mn max % P max % S max %
DC01 Commercial quality 0.12 0.60 0.045 0.045
DC03 Drawing quality 0.08 0.45 0.030 0.030
DC04 Deep drawing quality 0.08 0.40 0.025 0.025

Mechanically, the family is specified by a tensile strength band and a minimum elongation that move in opposite directions as the grade number rises. DC01 is quoted at roughly 270–410 MPa tensile strength with a minimum elongation of 28%, while DC04 drops to about 270–350 MPa with a minimum elongation of 38% and a distinctly lower yield point. In trade language DC01 is often called CR4, the older cold-reduced designation used in the United Kingdom, and DC04 is the grade selected when a component must survive a deep draw without splitting. DC02 and DC05 are the intermediate and extra-deep-drawing options in the same series, and the older DIN 1623 designations St12, St13 and St14 correspond approximately to DC01, DC03 and DC04.

St37 and Its Current Equivalent

DIN 17100 St37-2 specified a minimum yield strength of 235 MPa and a tensile strength range of roughly 340–470 MPa for thin sections. When DIN 17100 was withdrawn in favour of EN 10025-2, St37-2 was replaced by S235JR. In that designation the figure 235 repeats the minimum yield strength in MPa, the letter J indicates a minimum impact energy of 27 J tested at 20 °C, and R indicates the room-temperature toughness class. Material certified to EN 10025-2 is therefore the correct modern substitute whenever a legacy drawing still calls out St37. Grades such as St37-3U, which required impact testing at lower temperatures, map onto S235J0 or S235J2 according to the test temperature demanded.

A36: American Structural Carbon Steel

ASTM A36/A36M is a structural specification rather than a forming specification. Its chemistry limits are broad - carbon up to about 0.26%, manganese up to 1.20% with a specified minimum in heavier sections, phosphorus limited to 0.04% and sulphur to 0.05% - and the grade is defined mainly by its mechanical requirements: a minimum yield strength of 250 MPa and a tensile strength range of 400–550 MPa. A36 is normally supplied hot rolled. Although it can be cold reduced for special orders, it is not a substitute for DC01 in a drawing operation, because the higher carbon and manganese content lowers ductility and the surface is not controlled for forming.

Surface Condition, Tolerances and Coil Delivery

Cold-rolled grades such as DC01 are supplied with a matte or bright finish, normally oiled to prevent rust in transit, with thickness tolerances and flatness defined by EN 10131. Hot-rolled grades such as S235JR and A36 are commonly supplied to EN 10051 or ASTM A6/A6M tolerances, either as black hot-rolled coil or as pickled and oiled coil, with mill edge or trimmed edge according to the customer's slitting and blanking equipment. Coil inner diameter is usually 508 mm or 610 mm, and standard coil weights run from about 4 t to 6 t depending on the line. Cold-rolled carbon coil is typically available from around 0.3 mm to 3.0 mm thick, while hot-rolled structural coil begins at roughly 1.5 mm and goes upward.

Choosing the Right Grade for the Job

Deep-drawn panels, enclosures and components - choose the cold-rolled family, DC01 for simple bends and DC03 or DC04 where the draw ratio is demanding.

Welded frames, brackets and general structures - choose S235JR where European drawings apply, or A36 where American drawings apply.

Parts that will be galvanized or painted - DC01 with a controlled surface is preferred, since formability and coating adhesion are both predictable.

Thick, load-bearing plate converted from coil - A36 or S235JR is appropriate; a drawing grade would be over-specified and wasteful.

Frequently Asked Questions

Q: Is DC01 the same as CR4?
In trade use they are treated as equivalent. CR4 is the older cold-reduced mild steel designation, and DC01 is the EN 10130 grade that now covers the same commercial-quality, cold-rolled product.

Q: What is the difference between DC01 and DC04?
DC04 is a deep-drawing grade with tighter limits on carbon, manganese, phosphorus and sulphur, plus higher elongation and a lower yield point. It forms more complex shapes without splitting but costs more than DC01.

Q: Can St37 still be ordered today?
Yes, but it is normally supplied as its EN 10025-2 equivalent S235JR. Legacy drawings calling out St37-2 should be updated, and inspection certificates will quote the S235JR designation.

Q: Is A36 suitable for cold forming?
Only for mild forming such as simple bending with generous radii. For deep drawing or severe forming, a cold-rolled DC-grade coil should be used instead.

Q: Which thicknesses are available for DC01 carbon steel coil?
Cold-rolled DC01 coil is typically produced from about 0.3 mm to 3.0 mm, with width and edge condition set by the slitting arrangement agreed on the order.

Q: Can DC01 be galvanized or painted after forming?
Yes. DC01 is a common substrate for hot-dip and electro-galvanized products and takes paint well, provided the surface is clean, dry and free of oil or white rust before processing.