Two Designation Systems for Cold-Rolled Low-Carbon Coil
Cold-rolled flat product is bought against one of two grade families in most international projects. The European family is laid down in EN 10130 and runs from DC01 to DC06; the Japanese family is laid down in JIS G 3141 and runs from SPCC through SPCD to SPCE. Both systems describe unalloyed, cold-reduced sheet and strip with a clean and reasonably level surface, but they grade formability differently and apply different chemical ceilings, so a quotation must state which system governs.
EN 10130 superseded the former national designations, which is why the old marks St12, St13, St14 and St15 still appear on legacy drawings and are now written DC01, DC03, DC04 and DC05. The same base grades reappear in the coated-product standard EN 10152 with a ZE prefix, and the informal trade label CR4 is still widely used for commercial-quality cold-reduced mild steel.
Chemical Composition Limits in EN 10130
Formability in a low-carbon aluminium-killed or interstitial-free analysis is governed mainly by carbon, manganese, phosphorus and sulphur, all held down to raise the plastic strain ratio. The table below gives the maximum values specified for the three most frequently traded grades.
| Grade | C max % | Mn max % | P max % | S max % | Typical forming duty |
|---|---|---|---|---|---|
| DC01 | 0.12 | 0.60 | 0.045 | 0.045 | Bending, coining, beading, light drawing |
| DC03 | 0.10 | 0.45 | 0.035 | 0.035 | Deep drawing and difficult profiling |
| DC04 | 0.08 | 0.40 | 0.030 | 0.030 | Severe deep drawing, panels and shells |
| DC05, DC06 | Tighter carbon and phosphorus ceilings are set in the standard table; these grades are ordered against plastic strain ratio and strain-hardening values rather than chemistry alone | Extra deep drawing, complex geometries | |||
Grades above DC04 are normally quoted by plastic strain ratio r90 and strain-hardening exponent n90 in addition to composition, because the useful forming reserve of a very low-carbon, titanium or niobium stabilised analysis is no longer visible from chemistry alone.
Mechanical Properties of the Base Grades
EN 10130 fixes yield and tensile windows rather than single minimum values, which keeps the material drawable and prevents an over-strong delivery from splitting in the press. The figures below are the values applied to the base grades without metallic coating.
| Grade | Yield strength Re MPa | Tensile strength Rm MPa | Elongation A80 min % |
|---|---|---|---|
| DC01 | 140 - 280 | 270 - 410 | 28 |
| DC03 | 140 - 240 | 270 - 370 | 34 |
| DC04 | 140 - 210 | 270 - 350 | 38 |
The pattern is deliberate: as the grade number rises, the tensile window narrows and the elongation floor rises, so a DC04 delivery cannot legally be as strong as a DC01 delivery. A coil that is stronger than its grade allowance will spring back and tear at tight radii even though its elongation test passes.
SPCC Under JIS G 3141 and Its Practical Equivalents
SPCC is the commercial-quality cold-reduced carbon steel sheet and strip of JIS G 3141, with SPCD and SPCE sitting above it for drawing and deep drawing. The composition of SPCC is deliberately looser than that of DC01 - carbon to 0.15%, manganese to 0.60%, phosphorus to 0.100% and sulphur to 0.050% - and the specified tensile strength floor is 270 MPa. In practice SPCC is used for brackets, enclosures, ducts and general stampings where surface finish matters more than draw depth.
A purchaser replacing SPCC with DC01, or the reverse, should treat the two as close but not identical: a DC01 coil with 0.045% maximum phosphorus is the cleaner and more consistent forming stock, while an SPCC coil bought on the lower price band can carry phosphorus levels that a DC-grade order would reject. Where a part is drawn in a single pass and the tool was validated on SPCC, switching suppliers without confirming chemistry is the usual cause of split flanges.
Coil Presentation, Tolerances and Surface Condition
Cold-rolled coil is supplied with thickness tolerances set in EN 10131 for uncoated and electrolytically coated product, and flatness tolerances in the same standard. Widths are normally trimmed to a fixed mill edge, and the delivered coil is identified by grade, heat number, coil number, nominal thickness and width, plus the mass and inside diameter of the eye. Oiling with a rust-preventive film is normal practice; a dry coil is supplied only on request and needs a controlled store.
Surface condition is quoted separately from grade. Commercial surface quality permits minor imperfections that do not affect forming, while the improved classes are intended for exposed parts and require a defect count agreed between the mill and the user. Printing, laser marking or a paper interleaf is used where the surface will be seen after forming.
Selecting a Grade by Forming Severity
Grade selection is driven by the strain the part imposes, not by the product name. Bends, beads and coinings are within the capacity of DC01 or SPCC. A single deep draw with a moderate draw ratio needs DC03. Multiple draws, small punch radii, high dome heights or a visible outer panel need DC04 and above. Where the part is subsequently hot-dip coated, the forming grade must still satisfy the drawing tool, because galvanizing does not restore lost ductility.
Two further rules reduce claims: keep the coil within one heat for a critical run where the press is set close to the forming limit, and record the actual yield strength of the delivered coil against the grade window. Forming behaviour tracks the position inside the window far more closely than it tracks the grade label.
Frequently Asked Questions
Q: Is DC01 the same as SPCC?
A: No. They come from different standards with different limits. DC01 is defined in EN 10130 and SPCC in JIS G 3141; SPCC permits higher phosphorus and sulphur, so it is the more forgiving but less consistent specification for deep forming.
Q: What does the number after DC mean?
A: It ranks formability. A higher number indicates a lower-carbon, higher-ductility material intended for deeper forming, so DC04 will draw where DC01 would tear.
Q: Can DC04 be substituted for DC01?
A: Substituting upward is technically safe - DC04 will form anything DC01 forms - but it costs more and can show a softer surface that marks in handling. Substituting downward, from DC04 to DC01, is not acceptable on a validated deep-drawing tool.
Q: What thickness and width range is normally available?
A: Cold-rolled coil is commonly produced from about 0.3 mm to 3.0 mm in width from 600 mm up to 1500 mm, with 1000 mm, 1219 mm, 1220 mm and 1250 mm as the usual mill widths before slitting.
Q: How should a cold-rolled coil be stored?
A: Keep it indoors on timber or rubber bearers clear of the floor, away from condensation and acid or alkali fumes, and consume the oldest heat first. An unoiled coil can show edge rust within weeks in a humid store.
Q: Does the coil need oil for shipment?
A: A rust-preventive oil film is standard for sea freight and is normally kept thin enough to be welded or formed without degreasing; specify a dry coil only if your process cannot tolerate oil.
Q: Which grade is used for appliance and automotive panels?
A: Exposed panels are normally ordered in DC04 and above, or in the equivalent interstitial-free deep-drawing grades, because the visible outer skin needs both drawability and a controlled surface.