What are the chemical composition requirements for DC06?
Its characteristics include low carbon (C≤0.008%, or even lower), low manganese, phosphorus, and sulfur, and a certain amount of aluminum (Alt≥0.015%). The extremely low carbon content is key to ensuring its excellent stamping performance.
What is the typical mechanical property range of DC06?
Taking a thickness of 0.5~0.7mm as an example:
Yield strength: 110~170 MPa
Tensile strength: ≥260~270 MPa
Elongation after fracture: ≥39% (some requirements can reach ≥41%, and even ≥45% through process optimization)
Plastic strain ratio r90 value: ≥2.1 (thickness 0.5~<1.0mm)
Work hardening index n90 value: ≥0.22 (thickness 0.5~<1.0mm)
Why is the elongation of DC06 important?
Higher elongation indicates stronger plastic deformation capacity of the material, allowing it to withstand greater deformation during stamping without cracking. For example, when high user requirements are needed, elongation can reach ≥45%.
What are the r-value and n-value of DC06?
r-value (plastic strain ratio): Measures the sheet's resistance to thinning. A higher r-value indicates better deep-drawing performance.
n-value (work hardening index): Reflects the material's ability to increase strength during plastic deformation. A higher n-value indicates stronger resistance to localized concentrated deformation, which is beneficial for uniform deformation.
Does DC06 have an aging hazard?
As an IF steel, DC06 does not have an aging hazard; its properties do not change significantly with storage time.