Dx51d+Z Galvanized Iron Steel Corrugated and Roofing Sheet Coil

Nov 10, 2025 Leave a message

What are the reasons for poor adhesion and easy peeling of galvanized layers?

High silicon content in the substrate can lead to an excessively thick alloy layer; excessively rapid cooling can generate internal stress; incomplete pretreatment can also affect adhesion. High-silicon steel can be pre-plated with nickel, using stepped cooling and enhanced pre-plating degreasing and pickling treatments.

How are white rust and black spots formed on galvanized sheets?

Black spots are the result of further oxidation of white rust. White rust originates from poor passivation, lack of surface oiling, or residual moisture. It may also be caused by moisture, rain, or contact with corrosive media during transportation and storage.

How long can hot-dip galvanized sheets be stored in a warehouse?

The maximum storage time is three months. Prolonged storage can easily lead to oxidation due to environmental factors, resulting in defects such as white rust, affecting product quality.

What are large and small zinc spangles?

Large zinc spangles, also known as normal zinc spangles, are formed by the natural condensation of the zinc layer after galvanizing. Small zinc spangles are formed through controlled condensation and are smaller than normal zinc spangles, usually difficult to distinguish with the naked eye.

What is the protective principle of hot-dip galvanized layers?

First, it provides physical isolation, with the zinc coating preventing the steel from contacting the corrosive medium; second, it provides electrochemical protection, as the zinc electrode potential is lower than that of iron, and zinc preferentially corrodes in corrosive environments, protecting the steel substrate from corrosion.