High Quality ASTM Hot/Cold Rolled A283 A36 Grc A285 Grade C Cold/Hot Rolled Carbon/ASTM A240 304 316 321 201 2205 316L Stainless/Galvanized Steel Plate

Apr 13, 2026 Leave a message

Why is SPCC prone to rust?

Unprotected, low-carbon steel, exposed to air/water; factory coated with anti-rust oil.

SPCC storage requirements?

Dry, ventilated, moisture-proof, protected from acids and alkalis.

Common corrosion protection methods for SPCC?

Zinc plating (SECC/SGCC), spraying, electrophoresis, phosphating, passivation.

Does SPCC have a tensile strain mark warranty period?

No warranty (SPCD 3 months, SPCE 6 months).

SPCC pricing?

Mid-to-low end, high cost-performance ratio; lower than SECC/SGCC/stainless steel.