What is the yield strength requirement?
A: ≤280MPa (at room temperature), ensuring plasticity during molding.
What is the minimum elongation standard (A80mm)?
A: ≥30%, some high-grade products can reach over 35%.
What are the specifications for galvanized layer thickness?
A: Common thicknesses are 60g/m² (double-sided), 80g/m², 100g/m², and 120g/m². Higher coatings can be customized upon request.
What is the sheet thickness tolerance range?
A: Standard thickness is 0.5-3.0mm, tolerance ±0.05-±0.15mm, conforming to EN 10130 standard.
What are the surface quality grades?
A: Common grades are FB (normal surface), FC (higher grade surface), and FD (high-grade surface), each suitable for different appearance requirements.