Q195, Q215, Q235 and Q355 are Chinese structural steel grades frequently requested for shipbuilding and bridge projects. Buyers sometimes write them together with an ASTM prefix, as in ASTM Q215A, which is a mix-up: the Q grades are defined by the GB system, and their US counterparts are different designations such as A36 or A572. This guide explains the GB grade series, where each grade fits in ship and bridge structures, and which certification applies when hull or bridge members are load-bearing.
Reading the Q designations
Q stands for yield strength in the Chinese system. The number after Q is the minimum yield strength in MPa at the reference thickness, so Q195 guarantees 195 MPa, Q235 guarantees 235 MPa and Q355 guarantees 355 MPa. The letter suffix A, B, C or D indicates the Charpy impact requirement: A carries no impact guarantee, B is tested at 20 C, C at 0 C and D at -20 C. For bridges and cold regions, C and D suffixes are the relevant choices.
| Grade | Standard | Min yield (t ≤ 16 mm) | Tensile strength | Typical duty |
|---|---|---|---|---|
| Q195 | GB/T 700 | 195 MPa | 315-430 MPa | Light sections, ancillary parts |
| Q215 | GB/T 700 | 215 MPa | 335-450 MPa | General light structures |
| Q235 | GB/T 700 | 235 MPa | 370-500 MPa | Buildings, non-load-bearing ship and bridge parts |
| Q355 | GB/T 1591 | 355 MPa | 470-630 MPa | Primary welded structures |
Shipbuilding: general structural versus hull structural steel
For ship equipment, ladders, foundations, brackets and non-hull members, Q235 and Q355 are common and economical choices. Hull structural members are a different matter: they must comply with classification rules and be made from hull grades such as GB 712 (Chinese practice) or ASTM A131 (US practice), with designations A, B, D and E defined by Charpy toughness. A Q355 plate cannot replace a hull grade in a classed structure without the approval of the classification society, and the mill certificate must be endorsed accordingly. Buyers should therefore separate the hull package from the general equipment package in the enquiry.
Bridge construction
Load-bearing bridge girders in Chinese practice are specified to GB/T 714, the bridge structural steel standard, which uses q-series grades such as Q345q, Q370q and Q420q with specified low-temperature impact energy. The Q grades of GB/T 700 and GB/T 1591 serve auxiliary bridge parts: railings, walkways, supports, covers and temporary works. In international bridge projects, S355J2 or S355K2 (EN 10025-2) is the common alternative to Q355, and the Charpy temperature class must be matched to the site climate.
Mechanical properties and testing
The guaranteed values for the four grades follow the pattern of international structural steels: yield and tensile are verified by tensile tests, ductility by bend tests, and toughness by Charpy impact tests where the suffix requires it. For plates above 40 mm, through-thickness properties and carbon equivalent become part of the specification. The comparison points for international buyers are: Q235 approximates S235JR (EN 10025-2) and A36 (ASTM A36) at the same strength level, while Q355 approximates S355JR (EN 10025-2) and A572 Grade 50 (ASTM A572).
Welding and documentation
Q235 and Q355 weld with standard processes and consumables; preheating of 100-150 C is common for Q355 above 25-30 mm thickness. Export documentation should include a mill certificate with heat number, chemical composition, mechanical results and the standard edition, plus third-party inspection where the contract requires it. For classed hull steel, the certificate must carry the classification society stamp and the full traceability chain from ladle to plate.
Frequently Asked Questions
What is the difference between Q235 and A36? Both guarantee roughly 235-250 MPa yield and a similar tensile range, but they are issued under different standards with different tolerances and inspection rules. For non-critical structures they are often substituted; for classed or specified structures the governing standard must be followed.
Is Q355 the same as S355? Similar strength level, different standards: Q355 is written to GB/T 1591 and S355 to EN 10025-2. The Charpy suffix must also be matched: Q355C/D correspond approximately to S355J0/J2 in impact performance.
or Q215 for light structures? Both are low-strength economy grades. Q195 is used for light sections and cold-formed members, Q215 for slightly heavier general duty. Neither is intended for primary welded structures.
What does GB 712 cover? GB 712 is the Chinese standard for hull structural steel plates, covering grades A, B, D and E with Charpy test temperatures of 20 C, 0 C, -20 C and -40 C respectively. It is the Chinese counterpart of ASTM A131 for classed ship hulls.
Which grade should be used for ship hull plating? Hull plating must use classification-approved hull grades to GB 712 or ASTM A131, selected by the rule stress level and the service temperature. Ordinary Q235 or Q355 cannot be substituted without class approval.
What tests are required for bridge plates? Typical requirements are tensile testing, Charpy impact at the specified temperature, bend testing, and ultrasonic examination for thick plates, executed to GB/T 714 or the governing project standard, with the results recorded on the mill certificate.