SPCC-SD and DC01 are among the most frequently traded cold-rolled carbon steel grades in the world, and the same product family appears in every standard system: SPCC under JIS G3141, DC01 under EN 10130, St12 under DIN 1623 and CS under ASTM A1008. This article explains what the designations mean, what SPCC-SD adds to plain SPCC, how the grades compare, and how to select between DC01 and DC04 when the forming gets harder. The practical thickness range for this product family is 0.1-3.0 mm with widths from 300 to 1600 mm, which covers most enclosure, panel, furniture and light structural work.
SPCC and SPCC-SD: what the letters mean
SPCC stands for Steel Plate Cold Commercial in the JIS G3141 system, the commercial-quality cold-rolled carbon steel. The letters SD describe the delivery condition: the sheet is skin-passed, temper rolled after annealing, which gives a flatter and smoother surface and prevents the yield-point elongation that causes stretcher strains in forming. In practice SPCC-SD is the condition most sheet buyers need, because it arrives flat and forms cleanly. Plain annealed SPCC without skin pass is softer but can show fluting on bending, so it is less common in sheet trading.
Grade comparison in one table
| Property | SPCC (JIS G3141) | DC01 (EN 10130) | DC03 (EN 10130) | DC04 (EN 10130) |
|---|---|---|---|---|
| Carbon, max | 0.12% | 0.12% | 0.10% | 0.08% |
| Manganese, max | 0.50% | 0.60% | 0.45% | 0.40% |
| Yield strength Rp0.2 | Not specified | 140-280 MPa | 140-240 MPa | 140-210 MPa |
| Tensile strength | 270 MPa min | 270-410 MPa | 270-370 MPa | 270-350 MPa |
| Elongation A80, min | Per thickness band | 28% | 32% | 36% |
The elongation figures for the DC grades apply to the 0.4-2.0 mm thickness band; other bands have slightly different limits, so compare on the actual certificate. SPCC guarantees elongation per thickness band rather than a single value, which is why the certificate is the reference for a JIS order.
DC01 vs DC04: when to move up
DC01 is the basic bending and simple stamping grade: it folds, embosses and flanges without trouble, and it is the default for enclosures, brackets, panels and general sheet metal. DC03 adds a lower carbon limit and better stretchability for medium drawing. DC04 is the drawing grade of the family: lower carbon, lower yield, higher elongation, and the ability to accept a deeper draw without splitting. The rule of thumb is to start with the cheapest grade that passes the forming trial: DC01 for bends and shallow forms, DC03 for moderate drawing, DC04 for deep cups and complex panels. Upgrading a grade costs less than retooling after a split part, so when a design sits at the edge of a grade, move up one step.
Surface, tolerances and delivery condition
For the 0.1-3.0 mm thickness range, surface quality and flatness matter as much as chemistry. Specify the surface class you need, and for parts that will be painted or powder coated without filler, ask for the tighter surface class with skin-passed delivery. Thickness and width tolerances follow the ordered standard, JIS G3141, EN 10130 or ASTM A1008, and the tolerance class should be stated in the inquiry, not assumed. Sheets can be supplied cut-to-length from coil, with trimmed or mill edges, and with an oiled or dry surface. For export, confirm the packaging level and, if you process coils on your own line, the inner diameter.
Frequently asked questions
1. What does SPCC-SD mean?
SPCC is the commercial-grade cold-rolled carbon steel of JIS G3141. SD marks the skin-passed delivery condition: annealed, then temper rolled for flatness and a smooth surface, which prevents stretcher strains in forming.
2. Is DC01 the same as SPCC?
They are close but not identical. Both limit carbon to 0.12%, but DC01 (EN 10130) guarantees a yield range and a minimum elongation of 28%, while SPCC (JIS G3141) guarantees tensile strength and elongation per thickness band without a yield figure.
3. What thickness range is available?
The practical range for this product family is 0.1-3.0 mm in thickness and 300-1600 mm in width, supplied as coil or cut-to-length sheet.
4. When should I choose DC04 instead of DC01?
When the part is deep drawn or stretch-formed. DC04 has lower carbon, 0.08% max, lower yield and higher elongation, 36% min at A80, so it accepts deeper drawing without splitting.
5. Which standard should I order to?
Order to the standard your production and certificates require: JIS G3141 for SPCC, EN 10130 for DC grades, ASTM A1008 for CS, or DIN 1623 for St12. The grades are close enough for most jobs, but certify to the system your customer accepts.
6. Why does the sheet show surface marks after bending?
Yield-point elongation causes fluting on annealed-only material. Skin-passed delivery, SPCC-SD or the skin-rolled condition of the DC grades, prevents this, which is why SD is the standard sheet condition in trade.