How resistant are cold-rolled coils to chloride salt corrosion?

Jan 27, 2026 Leave a message

1.Why are chloride salts so corrosive?

Damage to passivation film: It can penetrate and destroy the fragile protective oxide film formed on the steel surface.

Formation of corrosion cells: It forms concentration cells in localized areas (such as scratches and crevices), triggering pitting and crevice corrosion, which is insidious and deep.

High conductivity: Chloride solutions have high conductivity, greatly accelerating the electrochemical corrosion process.

Hygroscopicity: Chloride salts (such as NaCl) readily absorb moisture from the air, forming an electrolyte film on the surface.

cold-rolled coil

2.How resistant are ordinary carbon steel cold-rolled coils to chloride corrosion?

Extremely poor. Without any protection, it rapidly forms red rust in chloride salt environments, with a very high corrosion rate.

cold-rolled coil

3.How resistant are hot-dip galvanized cold-rolled coils to chloride salt corrosion?

Good/Medium Sacrificial Anodic Protection: The zinc layer corrodes before the steel, providing electrochemical protection to the substrate. In chloride environments, the corrosion products of zinc (white rust) can slow the process to some extent, but the protection life depends on the thickness (weight) of the zinc layer and the severity of the corrosive environment.

cold-rolled coil

4.How resistant are hot-dip aluminized zinc cold-rolled coils to chloride salt corrosion?

Excellent

Barrier protection + sacrificial protection: Aluminum forms a dense alumina barrier layer, blocking corrosive media; zinc provides sacrificial protection at scratches. Its chloride corrosion resistance life is typically 2-6 times that of pure galvanized steel sheets of the same coating thickness.

 

5.What are the key influencing factors?

Chloride ion concentration: The higher the concentration, the faster the corrosion. Seawater, de-icing salt, and coastal atmosphere are all high-chloride environments.

Frequency of wet-dry cycles: This is the most severe condition. The cyclical wet-drying process concentrates salt and continuously provides oxygen, drastically accelerating corrosion (e.g., in tidal zones and splash zones).

Temperature and humidity: High temperature and high humidity environments greatly accelerate all corrosion processes.

Surface coating integrity: Any cuts or scratches on a coated product will become the starting point for corrosion, destroying the protective layer.