How to tell if galvanized steel coating needs maintenance or replacement?

Jun 17, 2025 Leave a message

1.What are the different situations of coating surface characteristics?

Normal zinc layer: silver-grey metallic luster, no obvious defects

White rust (zinc hydroxide): white powder or flocculent substance appears on the surface

Gray rust (zinc oxide): gray-white dense layer, zinc layer is exposed after wiping

Red rust (iron oxide): brown-red rust appears, and the zinc layer has penetrated into the substrate

Zinc layer peeling off: flaking off, exposing the steel matrix

Galvanized Steel

2.What are the weak points of the galvanized layer that are prone to corrosion?

Welding joints and heat-affected zones (temperature causes the zinc layer to become thinner);
Corners and gaps of components (water/dust accumulation easily forms galvanic cells);
Bolted joints (mechanical stress causes cracking of the coating);
Concealed areas such as buried/underwater (more severe environmental corrosion).

 

3.What are the testing tools and standards?

Magnetic thickness gauge: Determine the zinc layer thickness by measuring the change in magnetic flux;
Accuracy: ±1μm (applicable to 1-200μm zinc layer);
Destructive testing: Stripping method: Dissolve the zinc layer with chemical reagents, weigh and calculate the thickness;
Microscope method: Observe the zinc layer thickness after polishing the cross section, accuracy ±2μm.

Galvanized Steel

4.What are the key points for judging special scenarios?

Buried galvanized steel (cooperative judgment of cathodic protection) • Potential detection: Use copper/copper sulfate reference electrode, when the potential is >-0.85V (CSE), the zinc layer is in the state of anodic protection; if the potential is >100mV, it is necessary to check whether the anode block is invalid. • Soil resistivity: When >50Ω・m, the corrosion rate is reduced, but galvanic corrosion may occur (sacrificial anode is required).
Underwater galvanized steel (coating integrity judgment) • Visual inspection by divers: Focus on whether the coating at the weld and bolt is bubbling (bubble diameter >5mm needs to be repaired); • Ultrasonic thickness measurement: Detect once every 2 years in areas above 5 meters underwater, and once a year in areas below 5 meters (water flow erosion accelerates corrosion).

Galvanized Steel

5.What are the emerging detection technologies?

Infrared thermal imaging: The damaged part of the zinc layer dissipates heat quickly, and the corrosion risk can be identified through temperature difference (accuracy ±0.5℃);
Laser induced breakdown spectroscopy (LIBS): In-situ analysis of the zinc layer composition, when the aluminum content is less than 5%, the corrosion resistance decreases and attention should be paid;
UAV + AI visual inspection: Automated inspection of high-altitude components (such as transmission towers) with an identification accuracy of 0.5mm.