Q345, Q355, S235, S275 and A36: What Each Designation Means
Hot rolled carbon steel plate in the 3-6 mm thickness range is specified against different national standards depending on where the project is designed and built. Q235 and Q345/Q355 follow the Chinese standards GB/T 700 and GB/T 1591, S235JR and S275JR follow the European standard EN 10025-2, and A36 follows the ASTM specification. The number in each designation indicates the minimum yield strength in MPa: Q235 and S235 both guarantee 235 MPa, Q345 and Q355 guarantee 345-355 MPa, S275 guarantees 275 MPa, and A36 guarantees 250 MPa. When plates are traded and fabricated internationally, the buyer must map the ordered grade to the governing design code and confirm the equivalence on the mill test certificate before production starts.
Mechanical Properties of Q355 in 3-6 mm Plate
Q355 is the modern replacement for the older Q345 grade in GB/T 1591. In light plate the guaranteed values are: yield strength ReH of at least 355 MPa for thickness up to 16 mm, tensile strength Rm in the 470-630 MPa range, and elongation A of about 21% minimum as commonly published for Q355A/B in this thickness range, with the value decreasing slightly as thickness grows. Impact energy KV2 of 34 J is required at 0 degrees C for grade C, at -20 degrees C for grade D and at -40 degrees C for grade E; grades A and B carry no mandatory impact test. For a 3-6 mm plate ordered as Q355C, the mill certificate must show a Charpy V-notch result of at least 34 J at 0 degrees C on the longitudinal specimen.
Yield Strength versus Plate Thickness
| Thickness t (mm) | Yield ReH (MPa, min) | Tensile Rm (MPa) | Impact KV2 |
|---|---|---|---|
| t ≤ 16 | 355 | 470-630 | Grade dependent |
| 16 < t ≤ 40 | 345 | 470-630 | Grade dependent |
| 40 < t ≤ 63 | 335 | 470-630 | Grade dependent |
| 63 < t ≤ 80 | 325 | 470-630 | Grade dependent |
Designers must use the yield value that corresponds to the actual ordered thickness rather than the nominal 355 MPa figure. For a 3-6 mm plate the full 355 MPa applies, which is one reason thin sections are preferred where bending and weight matter.
Cold Bending: The d = 2a, 180-Degree Test
For Q355A and Q355B in thicknesses up to 16 mm, the standard cold bend test specifies bending a specimen through 180 degrees around a former whose diameter d equals twice the plate thickness (d = 2a), with no cracks allowed on the outer surface of the bend. In practice this means a 3-6 mm Q355 plate can be cold folded on a press brake with a punch nose radius of roughly twice the plate thickness without risking edge or surface cracks. Bending across the rolling direction is the more demanding orientation, so the test is usually performed on a transverse specimen; the bend line should be deburred before forming.
How the Grades Differ in Composition and Behaviour
Q355 obtains its strength from small additions of niobium, vanadium and titanium combined with fine-grain control, while Q235 and A36 are plain carbon grades with no alloying additions. S275JR adds a guaranteed 27 J Charpy requirement at 20 degrees C. The practical consequences are clear: Q345 and Q355 allow lighter sections for the same design load; A36 and Q235 are cheaper and easier to weld; and S275JR or S355JR are the natural defaults when the design follows EN 10025-2 and requires a documented impact test.
Selection Guidance for Buyers
1. Identify the design code: Chinese projects usually demand GB/T 1591 grades, European projects EN 10025-2 and US projects ASTM, and the drawing should state which one governs. 2. Confirm the impact requirement: heated structures, cold-weather sites and offshore applications need grades C, D or E, or the J2 suffix in the European system. 3. Verify the delivery condition: hot rolled, controlled rolled or normalized plate differ in toughness even at the same nominal grade. 4. Check the documents: the mill test certificate must show the standard and edition, grade, heat number, chemical analysis, tensile, impact and bend results, all traceable to the shipped pieces.
Frequently Asked Questions
Is Q355 the same steel as Q345?
Q355 replaced Q345 when GB/T 1591 was revised, with the nominal yield strength moving from 345 MPa to 355 MPa and chemistry limits adjusted. Existing drawings made for Q345 are usually covered by Q355 supply after the design engineer confirms the substitution.
What is the elongation of Q355B in thin plate?
Published values are about 21% minimum for Q355A/B in light sections such as 3-6 mm, with the exact figure depending on thickness and the standard edition applied at the producing mill.
Why does Q355C require an impact test at 0 degrees C?
The C suffix sets a Charpy V-notch requirement of 34 J at 0 degrees C, protecting welded structures operating in cold weather from brittle fracture. Grades D and E extend the same 34 J requirement to -20 and -40 degrees C.
Can 3-6 mm Q355 plate be bent 180 degrees without cracking?
Yes, provided the bend former diameter is at least twice the plate thickness and the bend line is clean and burr-free. This is exactly the condition verified by the d = 2a cold bend test.
How does ASTM A36 compare with Q355 for thin plate?
A36 guarantees 250 MPa yield and is a general-purpose carbon grade; Q355 offers roughly 40% more yield strength, allowing thinner or lighter sections wherever the design takes advantage of it.
What documents should accompany hot rolled plate delivery?
At minimum a mill test certificate with the standard, grade, heat number, chemical composition and the tensile, impact and bend test results. Third-party inspection can be arranged by agreement when the project requires it.