A coil order that names DX51D, S350GD, Z90, Z180, Z275 and aluminium-zinc in one line is asking for a complete material definition, because each term covers one decision: which base grade, what strength, what coating type and how much coating. This article separates the four decisions and shows how they combine. The rule that governs everything is simple: the base grade carries the mechanical performance, the coating type and class carry the corrosion life, and both must be stated on the certificate.
DX51D: the forming grade of EN 10346
DX51D is the base forming grade of EN 10346, a ductile and flexible steel for bending, profiling and moderately complex forming. For flat product from 0.35 mm to 3.0 mm it guarantees a yield strength of 140-300 MPa, a tensile strength of 270-500 MPa and a minimum elongation of 22%. It is the default grade for ducting, cable trays, roofing profiles and appliance panels, and it accepts the full range of coating classes from Z90 to Z275. Where the forming is deep rather than simple, the DX52D or DX53D step improves the drawing margin.
S350GD: the structural grade
S350GD is the structural member of the same family, specified when the panel must carry load. It guarantees a yield strength of 350-500 MPa, a tensile strength of 420-600 MPa and a minimum elongation of 16%, and it is used for purlins, solar mounting frames, structural profiles and load-bearing cladding. The strength comes from the base chemistry, not the coating, so a Z180 coating on S350GD protects a structure that would be oversized in DX51D. Forming is by roll forming and cold bending, not deep drawing, because the high yield leaves less ductility.
| Grade | Yield Rp0.2 | Tensile Rm | Elongation A80 | Typical use |
|---|---|---|---|---|
| DX51D | 140-300 MPa | 270-500 MPa | 22% min | ducting, profiling, panels, moderate forming |
| DX52D | 140-300 MPa | 270-420 MPa | 24% min | moderate forming, appliance parts |
| S350GD | 350-500 MPa | 420-600 MPa | 16% min | purlins, solar frames, structural profiles |
| S450GD | 450-600 MPa | 480-620 MPa | 12% min | high-load cold-formed sections |
Zinc coating classes: Z90, Z180 and Z275
The Z classes state the total zinc mass on both surfaces: Z90 is 90 g/m², Z180 is 180 g/m² and Z275 is 275 g/m², measured by triple-spot with a single-spot minimum. The coating class is the primary driver of corrosion life in a given environment, so the choice should follow the exposure: Z90-Z140 for indoor and painted applications, Z180 for normal outdoor atmospheres, and Z275 for exposed rural, industrial and coastal duty. A heavier coating costs more and is slightly less formable at tight radii, but on an outdoor structure it is the cheapest insurance against early rust.
aluminium-zinc: the AZ coating family
The AZ coating family is a hot-dip alloy of roughly 55% aluminium, 43.4% zinc and 1.6% silicon, applied by the traditional hot-dip process. The aluminium gives the surface a long-lived barrier and a heat-reflective character, while the zinc content preserves sacrificial protection at cut edges, and the silicon controls the alloy reaction. AZ-coated coil is used for roofing and cladding, appliances, agricultural equipment and several non-exposed automotive components, and it is specified as AZ100, AZ150 or AZ185 according to the coating mass in g/m². The general rule is that a higher AZ class gives a longer service life in the same environment, so the class should be matched to the design life rather than chosen by habit; the coating mass on the certificate is the number that counts.
Choosing the right combination
Define the environment first: dry interior allows light zinc classes or an AZ class sized for the design life; outdoor exposure calls for Z180-Z275 or AZ150-AZ185; marine and industrial chloride atmospheres justify the top of both ranges. Then define the forming: roll forming and bending accept both DX51D and S350GD, deep drawing needs DX52D or DX53D, and load-bearing sections need the structural grades. Finally state the finish, the surface quality class and the passivation, and require the certificate to name the standard, the grade, the coating type and the measured coating mass, because those four items decide both the performance and the acceptance of the coil.
Frequently asked questions
What is the difference between Z90 and Z275 coating?
The total zinc mass on both surfaces: 90 g/m² against 275 g/m², so the heavier class carries roughly three times the zinc and gives a correspondingly longer corrosion life in the same environment.
What does aluminium-zinc mean?
aluminium-zinc is the trade description of the aluminium-zinc coating family, roughly 55% aluminium, 43.4% zinc and 1.6% silicon, applied by hot-dip and specified in EN 10346 as AZ classes.
Is DX51D suitable for deep drawing?
For moderate forming it works; for deep drawing, DX52D or DX53D gives a better margin, with lower yield and higher elongation, and the coating class should be kept light to avoid cracking at tight radii.
When should I choose S350GD instead of DX51D?
When the part must carry load: purlins, frames, solar mounting and structural profiles use S350GD or higher, which guarantee a yield of 350 MPa and above, while DX51D covers non-load-bearing panels and ducting.
What is the difference between AZ100 and AZ150?
The coating mass: AZ100 is 100 g/m² and AZ150 is 150 g/m² on both surfaces; in the same atmosphere the heavier class generally gives a longer service life, so choose the class from the design life and verify the certificate.
Which is better for roofing, Z275 or AZ150?
Both serve outdoor roofing; Z275 gives classic pure-zinc sacrificial protection, while AZ150 adds the aluminium barrier and heat reflectivity of the AZ family; the choice depends on the atmosphere, the roof design and the local specification.