SECC Material Properties: Electrolytically Zinc-Coated Steel Sheet Explained

Aug 12, 2025 Leave a message

What SECC Steel Is

SECC is the designation for electrolytically zinc-coated cold-rolled steel sheet regulated by JIS G 3313. The substrate is a commercial or drawing quality cold-rolled sheet such as SPCC, SPCD or SPCE defined in JIS G 3141. Zinc is deposited from an electrolyte rather than from a molten bath, so the coating is thin, uniform and free of the spangle pattern that appears on hot-dip galvanized sheet. Coating mass is quoted in grams per square metre per side; commercial production typically covers roughly 10 to 40 g/m2 per surface, with 20 g/m2 the usual starting point for enclosures and appliances. Designations in this family carry an E prefix, and the number indicates grams of zinc per square metre per side.

Coating Structure and Passivation Chemistry

Layer Typical thickness or mass Function
Zinc coating 10 to 40 g/m2 per side, about 1.4 to 5.6 micrometres Cathodic, sacrificial protection of the steel
Passivation film Chromate film in the region of 0.1 to 1.0 mg/m2 expressed as chromium Suppresses white rust and anchors paint
Optional oil film 0.5 to 2 g/m2 Lubrication for stamping and temporary rust protection

The conversion between mass and thickness follows directly from the density of zinc, 7.14 g/cm3, so 10 g/m2 per side is about 1.4 micrometres. Traditional passivation relied on hexavalent chromium, which is now restricted: Directive 2011/65/EU limits hexavalent chromium to 0.1% by weight in homogeneous materials, and the REACH regulation imposes an equivalent control on articles placed on the European market. Trivalent chromium passivation and chromium-free systems based on silane or molybdate chemistry are the standard replacements, and both tend to reduce the maximum salt spray performance that electrogalvanized sheet can reach.

Mechanical Properties Are Set by the Substrate

The mechanical properties of SECC are those of the underlying cold-rolled substrate, because a coating a few micrometres thick does not carry load. A commercial quality substrate such as SPCC gives tensile strength in the 270 to 440 MPa band depending on temper and thickness, yield strength of roughly 140 to 280 MPa, and total elongation of 30% or more in the annealed condition. A high-strength substrate such as SAPH440 raises tensile strength into the 440 to 980 MPa range with yield strength from 280 to 590 MPa and correspondingly lower elongation. A specification should therefore name the substrate grade first and the coating second; the coating designation alone says nothing about strength.

Formability, Welding and Paintability

Because the coating is thin and metallurgically bonded, SECC stamps and bends more cleanly than hot-dip galvanized sheet of comparable corrosion performance. Flaking at tight bend radii is uncommon, although powdering can appear when a heavy coating is worked hard. Resistance spot welding is practicable, but zinc at the interface raises contact resistance and encourages porosity and electrode wear, so welding schedules need higher electrode force and more frequent tip dressing than uncoated SPCC. The passivation film is micro-porous, which is precisely what makes it a good paint base: powder coating, electrophoretic coating and screen printing adhere without an extra pretreatment step. The continuous zinc layer also provides effective electromagnetic shielding for electronic enclosures.

Corrosion Performance and Its Limits

Zinc protects steel in two ways at once, as a barrier and as a sacrificial anode. A scratch that exposes the substrate remains protected as long as zinc is present alongside it, which is not true of a purely organic coating. The practical limits are coating mass, edge condition and environment. Chromium-free passivation is more sensitive to humidity in storage than chromate, and a coil kept in a damp warehouse can develop white rust between the laps within a few weeks. Neutral salt spray results are quoted as time to red rust, generally 48 to 120 hours to ISO 9227, and the figure should always be read together with the coating mass and the passivation type.

SECC Compared with SPCC and Hot-Dip Galvanized Sheet

Property SECC SPCC, uncoated Hot-dip galvanized
Coating Electrolytic zinc plus passivation None, oil film only Hot-dip zinc, typically Z100 to Z275 designations
Appearance Uniform matt silver, no spangle Bright mill finish Visible spangle unless skin-passed
Corrosion protection Good for indoor and sheltered use Requires painting Strongest of the three, suited to outdoor exposure
Forming and welding Excellent for precision stamping and bending Excellent, easiest to weld Good, heavier tool wear, thicker coating

Typical Applications

SECC is selected where a clean, painted, electrically conductive and moderately corrosion-resistant surface is needed at low coating mass: computer and server chassis, hard drive brackets, power supply housings, copier and printer frames, appliance covers, automotive interior brackets, and any part that must be shielded against electromagnetic interference. It is a poor choice for continuously wet, salt-laden or high-temperature service, where a heavier hot-dip coating performs far better per unit of cost.

Frequently Asked Questions

Q: What does SECC stand for?
A: It is the designation for electrolytically zinc-coated cold-rolled steel sheet under JIS G 3313. The zinc is deposited from an electrolyte rather than from a molten zinc bath, which is why the coating is thin and free of spangle.

Q: Is SECC the same as hot-dip galvanized sheet?
A: No. SECC carries a thin electrolytic coating intended for indoor and painted applications, while hot-dip galvanized sheet carries a much heavier coating for exposed outdoor service.

Q: Can SECC be welded?
A: Resistance spot welding is used in production, but the zinc layer raises contact resistance, so electrode force must be increased and the tips dressed more frequently than when welding uncoated sheet.

Q: Does SECC rust at cut edges?
A: The zinc adjacent to a cut protects the exposed steel sacrificially, so edge rust develops more slowly than on uncoated sheet, but a heavy burr or a wide cut will still corrode in a humid environment.

Q: Which coating mass suits an appliance enclosure?
A: Most enclosures use 20 g/m2 per side with trivalent chromium or chromium-free passivation. Specify a heavier coating only where the part will see condensation or cleaning chemicals.