What are common rolling defects in cold-rolled coil production? How can they be avoided?

Sep 29, 2025 Leave a message

What are the core performance indicators of cold-rolled coil? What do they reflect?
Core performance indicators include:
Yield strength (σs): reflects the steel's ability to resist plastic deformation. Higher yield strength indicates harder steel, but also more prone to cracking during stamping.
Tensile strength (σb): reflects the maximum tensile force a steel can withstand before breaking, used to determine the material's load-bearing capacity.
Elongation (δ): reflects the steel's plasticity. Higher elongation makes it easier to stamp and bend (for example, DC04 has an elongation ≥38%, making it suitable for complex stampings).
Hardness (HV/HRB): reflects the hardness of the steel's surface. Higher hardness indicates better wear resistance but lower plasticity.
Surface roughness (Ra): reflects surface finish. Lower Ra values ​​(e.g., Ra ≤ 0.8μm) indicate a smoother surface, making it suitable for applications requiring a high aesthetic quality (such as appliance panels).


How is the thickness accuracy of cold-rolled coil measured? What equipment is commonly used?
Testing Method: Use a non-contact thickness gauge or contact micrometer. Specific Process:
Sampling: Take multiple specimens from different locations (head, middle, and tail) of the cold-rolled coil.
Testing: Non-contact thickness gauges (such as laser thickness gauges and X-ray thickness gauges) provide real-time online testing with an accuracy of ±0.001mm; contact micrometers are used for offline spot checks with an accuracy of ±0.002mm.
Determination: Compare the test value with the standard requirement (e.g., DC01 thickness deviation ±0.03mm). Any deviation outside this range is considered unqualified.


What is the "yield plateau" of cold-rolled coil? How does it affect subsequent processing?
The yield plateau refers to the stage in a tensile test where, after the stress reaches the yield strength, the stress stops increasing but the strain continues to increase (represented by the "flat" portion of the tensile curve). Impact on Processing:
Disadvantage: During stamping, the yield plateau can cause "slip lines" (Lüders lines) to appear on the steel plate surface, affecting the appearance (e.g., streaks on appliance housings).
Solution: Eliminate the yield plateau through a "flattening process" (light rolling to cause the steel to enter the plastic deformation stage earlier), or choose a low-carbon steel without a yield plateau (such as IF steel, interstitial-free steel).


How is the surface quality of cold-rolled coil tested? What are the criteria for determining this quality?
Inspection Method: Visual Inspection + Surface Defect Detection Instrument:
Visual Inspection: Observe the steel plate surface for defects such as scratches, pitting, oxidation discoloration, and inclusions under natural light or standard light (500mm from the surface, 45° viewing angle).
Instrumental Inspection: Online surface defect detectors (such as CCD camera inspection systems) can automatically identify defect type and size with an accuracy of 0.1mm.
Judgment Criteria: Refer to national standards (such as GB/T 13237-2023 "High-Quality Carbon Structural Steel Cold-Rolled Sheet and Strip"). The size and number of defects must meet the customer's grade requirements (e.g., "high grade" does not allow scratches larger than 0.3mm).
How does the "grain size" of cold-rolled coil affect performance? How is it detected?
Grain size refers to the size of the grains within the steel (expressed as "grain grade," with higher grades indicating smaller grains). Impact:
Smaller grains increase the steel's strength and hardness (fine grain strengthening), while also improving its plasticity and toughness (avoiding brittle fracture).
Excessively large grains result in uneven steel properties, making localized cracking more likely during stamping.
Testing method: Observe under a metallographic microscope: Cut a specimen → Grind and polish → Etch (with nital solution) → Observe the grain morphology under a microscope and compare it to a standard grain size chart to determine the grade (e.g., DC03 requires a grain size of ≥6).


What are common rolling defects in cold-rolled coil production? How can they be avoided?
Common defects and countermeasures:
Surface scratches: Caused by foreign matter on the rolls or impurities on the stock surface. Preventative measures: Clean the rolls regularly and strengthen stock surface inspection.
Waviness (edge ​​and center waves): Caused by uneven rolling force and inappropriate roll crown. Preventative measures: Adjust roll crown and optimize rolling force distribution.
Thickness deviation: Caused by fluctuations in rolling force and uneven stock thickness. Preventative measures: Use an automatic thickness control system (AGC) and strictly inspect stock thickness.