What Is DP Steel Used For? Dual Phase Steel Grades and Automotive Applications

Aug 19, 2024 Leave a message

What Dual Phase Steel Is

DP steel, short for dual phase steel, is a family of advanced high strength steels used mainly in car bodies. It is not a single grade but a group of grades defined by a tensile strength level, typically DP490, DP590, DP780 and DP980. Because dual phase sheet offers a high strength to weight ratio, it is one of the main materials that allows a body-in-white to be made lighter without losing crash performance.

The concept is straightforward. Instead of relying on alloying and a slow heat treatment to raise strength, the steel is cooled rapidly from the intercritical annealing temperature so that part of the microstructure transforms to hard martensite while the rest stays as soft ferrite. The result is a composite structure in a single sheet.

Microstructure and Strengthening Mechanism

The microstructure consists of a ferrite matrix with islands of martensite dispersed through it. Ferrite is soft and continuous, so it carries the deformation and gives the sheet its elongation. Martensite is hard and acts as the reinforcing phase.

Raising the martensite fraction directly raises tensile strength, which is why the grades are named after their minimum tensile strength. Within one strength level, producers can also vary the yield to tensile ratio to match a customer drawing requirement, because a lower ratio gives easier forming and a higher ratio gives better stiffness in service.

Grade level Reinforcing phase Main benefit
DP490 Low martensite fraction High elongation, easy forming
DP590 Moderate martensite fraction Balanced strength and formability
DP780 Higher martensite fraction Strength for structural members
DP980 High martensite fraction Crash energy absorption at low mass

Performance Characteristics of Dual Phase Sheet

Low yield strength relative to tensile strength, with a yield to tensile ratio generally between 0.5 and 0.65, which keeps the sheet easy to shape.

Elongation second only to TRIP steel within the advanced high strength group, so stretch forming remains practical.

A distinctive work hardening rate: strain concentrates in the soft ferrite, and in the low strain range of about 2 % to 3 % the yield strength rises quickly by roughly 140 to 220 MPa, giving a high initial instantaneous n value.

No yield point elongation, so the surface does not develop stretcher strains during forming and no temper rolling is required.

No ageing tendency, which means the forming behaviour stays stable in storage.

Bake hardening response up to about 30 to 150 MPa, so painted panels gain strength in the paint oven.

That hardening response matters in practice. A part is formed in the soft, ductile state and then stiffens as the coating is cured, so dent resistance improves without a sacrifice in formability at the press.

Where DP Steel Is Used in a Vehicle Body

Dual phase steel is the preferred grade for automotive structural parts, reinforcements and anti-collision components. Typical parts include:

Underbody cross members and floor reinforcements.

Longitudinal rails and rail reinforcements.

Bumper beams and bumper beam reinforcement structures.

B-pillar and door impact reinforcements, side members and seat mounting brackets.

Wheel arches and suspension mounting areas on some platforms.

The pattern is consistent: wherever a part must absorb impact energy or carry load while staying thin, a dual phase grade replaces a conventional mild steel at a higher strength level, or replaces a thicker, heavier part at the same strength. Weight reduction comes from gauge reduction, not from a change in the joining method, so existing spot welding lines can often be reused.

Forming, Welding and Processing Guidance

Forming DP steel is closer to forming a conventional high strength sheet than a mild steel. Springback is higher because the yield stress after forming is elevated, so tools usually need more compensation and, in some cases, a controlled draw bead or a post-stretch step. Blank holder force should be set high enough to suppress wrinkling in the flange while keeping the draw load inside press capacity.

Shear and trim edges are harder than on mild steel, so punch and die materials should be selected for higher contact pressure, and edge cracking should be checked on the trimmed blank before a die is released for production. For joining, resistance spot welding works well, but welding current and electrode force have to be re-optimised because of the higher electrical resistivity of the martensitic phase. Laser welding and structural adhesive bonding are both used in mixed-material body assemblies. Standard corrosion protection applies: galvanized DP grades such as DP590+Z or DP780+Z are common, and cut edges are usually sealed or protected by the paint system.

Frequently Asked Questions

Q: What does DP steel stand for?
DP stands for dual phase. The name describes the two-phase microstructure of ferrite and martensite that gives the sheet its combination of ductility and strength.

Q: What are the main grades of dual phase steel?
Grades are named by minimum tensile strength, most commonly DP490, DP590, DP780 and DP980. A higher number means a higher martensite fraction and higher strength with lower elongation.

Q: Why is the yield strength of DP steel low compared with its tensile strength?
The soft ferrite matrix starts to deform at a relatively low stress, so yielding begins early, while final strength is set by the martensite islands. A yield to tensile ratio around 0.5 to 0.65 makes the sheet easy to form while remaining strong in service.

Q: Does dual phase steel age or show yield point elongation?
No. DP steel has no yield point elongation and no ageing tendency, so it does not show Lüders bands on formed surfaces and its properties do not drift during storage.

Q: What is the bake hardening effect in DP steel?
After forming, the paint bake cycle at elevated temperature raises the yield strength by roughly 30 to 150 MPa. The gain improves dent resistance in outer panels without reducing the formability needed at the press.

Q: Can DP steel be welded on a normal spot welding line?
Yes. Resistance spot welding is the standard joining method, but current, electrode force and weld schedule should be re-qualified because of the higher resistivity of the martensitic structure, and electrode wear should be monitored.

Q: Which parts of a car body use dual phase steel?
It is used for structural and anti-collision parts such as underbody cross members, longitudinal rails, bumper beams, B-pillar reinforcements and seat mounting brackets, where energy absorption and low weight are both required.