The two substrate families
The substrate type determines the thickness, surface quality and application of the galvanized sheet. Cold-rolled galvanized sheet uses a cold-rolled steel substrate, typically 0.3-3.0 mm thick, with a smooth surface, high flatness and minimal thickness variation; it suits home appliances, automobiles and precision parts. Hot-rolled galvanized sheet uses a hot-rolled steel substrate, typically 3.0-12.0 mm thick, with surface scale that requires thorough pickling before galvanizing, slightly lower flatness and a lower cost; it suits construction panels such as roofing sheets and keels, and heavy machinery casings.
| Characteristic | Cold-rolled substrate | Hot-rolled substrate |
|---|---|---|
| Typical thickness | 0.3-3.0 mm | 3.0-12.0 mm |
| Surface | Smooth, uniform | Scale, needs pickling |
| Flatness and tolerance | Tight | Moderate |
| Cost | Higher | Lower |
| Typical uses | Appliances, cars, precision parts | Roofing, purlins, machinery |
Construction: why hot-rolled substrate dominates
Hot-dip galvanized (GI) sheets with hot-rolled substrates are the construction standard for roofing panels, wall panels and purlins. The reasons are practical. The wide thickness range from 3 mm to 12 mm meets different load requirements, for example about 5 mm for purlins and 0.8-1.2 mm for roofing panels. The zinc layer is heavy, typically 120-275 g/m2, giving strong outdoor corrosion resistance with less frequent maintenance. The cost is lower, with hot-rolled substrates roughly 20-30% cheaper than cold-rolled ones, which matters in large-scale construction. For high-end architectural panels, cold-rolled GI or EG substrates are used and coated with a film to enhance the appearance.
Home appliances: EG, cold-rolled GI and GA
The appliance industry demands high surface quality and formability, and three galvanized products are used. Electrogalvanized steel (EG) has a thin, smooth zinc layer deposited electrically; it paints easily and is used for refrigerator side panels and washing machine control panels in dry indoor environments. Cold-rolled hot-dip galvanized (GI) offers better corrosion resistance than EG at lower cost than GA, and is used for refrigerator back panels and air conditioner housings. Galvannealed (GA) has a fully alloyed zinc-iron coating; its weldability and scratch resistance suit high-frequency components, and it appears in high-end washing machine drums and compressor housings.
Automotive: why GA is preferred for bodywork
GA is the standard for painted body panels such as doors and hoods, and for chassis components. Three properties explain it. Weldability: the absence of a pure zinc layer prevents zinc splash and porosity during welding, which suits continuous spot welding lines. Paint adhesion: the alloyed zinc-iron coating bonds with paint noticeably better than pure zinc, reducing paint peeling, which is why carmakers specify GA for painted panels. Impact resistance: the moderate toughness of the alloy layer prevents flaking from vibration and small collisions. Some chassis parts, such as frames, use a heavy GI zinc layer above 275 g/m2 for enhanced resistance to stone-chip corrosion.
Storage rules that prevent white rust
Improper storage causes zinc oxidation and corrosion, and four points matter. Environmental control: store in a dry, well-ventilated room with relative humidity at or below 60%, away from rain and direct sunlight. Moisture-proofing: elevate sheets on wooden supports at least 10 cm above the floor so ground moisture cannot reach the zinc. Avoid overloading: stack flat sheets no higher than about 1.5 m and coils no more than three layers, to prevent deformation of the lower sheets and scratches on the zinc layer. Isolate from corrosion sources: keep material away from acidic and alkaline substances such as fertilizers and chemical raw materials. White rust can develop after 2-3 months in humid conditions; inspect regularly and wipe any white rust with a dry cloth in the early stage.
FAQ
Which galvanized sheet should be used for roofing?
Hot-dip galvanized (GI) with a hot-rolled or cold-rolled substrate depending on gauge: 0.8-1.2 mm roofing panels are usually cold-rolled substrate GI, while 3-12 mm purlins and heavy sections use hot-rolled substrate. Coating weights of 120-275 g/m2 cover most sites, with Z275 for coastal or industrial exposure.
What is galvannealed (GA) steel?
GA is hot-dip galvanized sheet that is heat-treated after galvanizing so the zinc and iron form a fully alloyed coating. The surface is matte grey, weldable, scratch resistant and paints well, which makes it the automotive bodywork standard.
What is electrogalvanized (EG) steel?
EG is cold-rolled sheet coated with a thin zinc layer by electrodeposition. The coating is smooth and uniform but thinner than hot-dip zinc, so EG is used indoors, mainly in appliances and electronics where paintability and surface quality matter more than maximum corrosion life.
Can cold-rolled galvanized sheet be used outdoors?
Yes, with an adequate coating weight. Cold-rolled substrate is fine for roofing and cladding in gauges up to about 1.2 mm, as long as the coating class matches the environment, Z180 inland and Z275 coastal or industrial.
Why does white rust form and how is it avoided?
White rust forms when moisture condenses on zinc and the surface cannot dry, typically between tightly stacked sheets or coils in humid storage. It is avoided by dry, ventilated storage, elevation above the floor, and chromium-free passivation at the mill.
What is the difference between GI and GA?
GI has a pure zinc coating, thicker and more protective, while GA has a fully alloyed zinc-iron coating that is thinner but welds and paints better. Use GI for corrosion life and GA for painted, welded, high-frequency applications.