What is the low temperature impact toughness of color coated coils?

Jul 29, 2025 Leave a message

1.How does coating material affect low temperature impact toughness?

Fluorocarbon coating (PVDF): Containing fluorine atoms in its molecular structure, it offers high bond energy and excellent molecular chain flexibility. It maintains excellent flexibility even at -40°C (as demonstrated by a low-temperature bend test: no cracking after a 180° bend at -40°C), making it the coating type with the best low-temperature impact toughness.
Silicon-modified polyester (SMP): Its low-temperature performance surpasses that of standard polyester, maintaining a certain degree of flexibility between -20°C and -30°C. However, its brittleness increases below -30°C, and microcracks may appear in bend tests.
Standard polyester (PE): Its low-temperature brittleness is more pronounced, with flexibility decreasing between -10°C and -20°C. The coating is susceptible to flaking or cracking when subjected to impact (such as hail or impact from hard objects).
Specially modified coatings: Some manufacturers improve the low-temperature toughness of coatings by adding plasticizers or adjusting the molecular structure (such as by introducing flexible segments). For example, "low-temperature resistant PE" can lower the brittle transition temperature from -15°C to -30°C.

Color coated coil

2.How does the substrate affect low temperature impact toughness?

The low-temperature impact toughness of the substrate (steel plate) is the "basic support" for the overall impact resistance of the color-coated coil, especially when the coating is damaged by impact, the toughness of the substrate can avoid overall fracture:
Hot-dip galvanized substrate (DX51D+Z): low-carbon steel is used, with good low-temperature toughness. The impact energy (Charpy V-notch) at -40℃ can reach more than 27J, which is suitable for cold areas.
Alu-zinc-coated substrate (AZ150): The aluminum-zinc alloy coating does not affect the toughness of the substrate itself. The toughness of the substrate is close to that of the galvanized substrate, but attention should be paid to the bonding strength of the coating at low temperatures (to avoid falling off due to impact).
Cold-rolled substrate (SPCC): If it is ordinary low-carbon steel, the low-temperature toughness is acceptable; if the carbon content is high (such as medium carbon steel), it is easy to become brittle at low temperatures and is not suitable for severe cold areas.

Color coated coil

3.How does the bonding strength between the coating and the substrate affect low-temperature impact toughness?

At low temperatures, the difference in thermal expansion coefficients between the coating and substrate can cause interfacial stress. If the bond strength is insufficient (cross-cut test grade <1), the coating can easily peel from the substrate during impact, exacerbating damage. For example, epoxy primers offer superior low-temperature adhesion to common polyester primers, better maintaining the bond between the coating and the substrate.

Color coated coil

4.How does it perform in actual scenarios?

In the northern winter (-10℃ to -30℃), fluorocarbon coated color coated coils can resist the impact of hail (diameter ≤2cm) without damage to the coating; ordinary PE coatings may have local cracks, and if water enters and freezes later, the coating will peel off more severely.
In high-altitude and cold areas (such as the Qinghai-Tibet Plateau, where the temperature drops to -40℃ in winter), PVDF coating + high-toughness substrate (such as Q235B low-carbon steel) must be selected, otherwise the color coated coils may crack during installation or use due to low-temperature brittleness.

 

5.What are the measures to improve reliability in low temperature environments?

Prioritize high-toughness coatings: PVDF fluorocarbon coatings are preferred in low-temperature environments (below -20°C), and ordinary PE coatings should be avoided; if the budget is limited, low-temperature modified SMP coatings can be selected (the results of the low-temperature bending test need to be confirmed).
Matching high-toughness substrates: Use low-carbon steel substrates (such as DX51D+Z, SPCC low-carbon grade) and avoid high-carbon substrates; if used outdoors (such as roofs and wall panels), it is recommended that the substrate thickness be ≥0.4mm to improve the overall impact resistance.
Control processing and installation links: When processing (such as bending and shearing) at low temperatures, avoid excessive force (such as reducing the bending angle and increasing the bending radius) to prevent the coating from cracking due to brittleness; reserve thermal expansion and contraction gaps during installation to reduce the impact of temperature stress on the coating.