What is the purpose of tempering carbon structural steel?

Aug 26, 2025 Leave a message

What is the purpose of tempering carbon structural steel?
Tempering carbon structural steel involves reheating the quenched steel to a temperature below Ac1 (typically 150-650°C, avoiding the critical decomposition zone of the quenched martensite), holding it for a specified period, and then slowly cooling it. Its core function is to correct post-quenching performance defects and "customize" the mechanical properties of steel according to requirements, ultimately achieving a balance of strength, hardness, toughness, and ductility. This can be categorized into the following five key functions:
1. Eliminating quenching internal stresses to prevent cracking or deformation in parts
The rapid cooling process during quenching can cause severe internal stresses within the steel. This is primarily due to two sources:
Tectonic stress: When austenite rapidly transforms into martensite, its volume expands (martensite is larger than austenite by volume). However, the uneven cooling rates of different parts of the part (such as the surface and core of thick-walled parts, or the edges and grooves of complex-shaped parts) cause asynchronous microstructural transformations and generate internal stresses.
Thermal stress: During rapid cooling, the temperature difference between the surface and core of the part is significant, causing the surface to shrink faster than the core, resulting in tensile and compressive stresses.
If these internal stresses are not eliminated, at best, they can cause deformation of the part during storage or processing (such as bending of shafts or warping of plates), or at worst, directly cause cracking (especially in high-carbon structural steel or large-cross-section parts). During tempering, atoms gain energy during heating, which can alleviate lattice distortion through diffusion and dislocation movement, gradually releasing internal stress.
For example, after quenching, the internal stress of 45 steel can reach hundreds of MPa. After low-temperature tempering at 200°C, this stress can be relieved by 50%-60%. After high-temperature tempering at 500°C, the stress relief rate can reach over 80%, fundamentally preventing component failure.
2. Reduce Brittleness and Improve Steel's Toughness and Plasticity
Although quenched carbon structural steel has extremely high hardness and strength, its martensite structure is a "supersaturated solid solution," resulting in severe lattice distortion and extremely high dislocation density. This results in extremely poor toughness and low plasticity. (For example, the impact energy absorbed by quenched 45 steel is only 5-10J, making it prone to brittle fracture when bent and unable to withstand impact loads.) This makes it virtually unsuitable for direct use as finished parts. One of the core functions of tempering is to reduce brittleness. During heating, supersaturated carbon precipitates from the martensite (forming carbides such as cementite), gradually alleviating martensite lattice distortion and reducing resistance to dislocation movement, significantly improving toughness and ductility.

For example, 45 steel has an impact energy absorption of approximately 8J after quenching (untempered). This energy increases to 15-20J after low-temperature tempering at 200°C (still somewhat brittle, but sufficient for low-impact applications). After high-temperature tempering at 550°C, the impact energy absorption reaches over 50J (significantly improving toughness and enabling it to withstand moderate impact).

For high-carbon structural steels (such as 65 steel), the plasticity improvement after tempering is even more pronounced, with elongation increasing from 1%-2% after quenching to 10%-15%, preventing parts from breaking easily when subjected to external forces.
3. Adjusting Hardness and Strength to Meet Different Application Requirements
After quenching, steel reaches peak hardness and strength (e.g., 45 steel reaches a hardness of HRC55-60 and a tensile strength of over 1000 MPa after quenching). However, not all applications require extreme hardness. Performance requirements for different parts vary greatly (e.g., tools require high hardness, shafts require a balance of strength and toughness, and connectors require plasticity). Tempering allows precise adjustment of hardness and strength by controlling the heating temperature:

Low-temperature tempering (150-250°C): Only a small amount of fine carbides precipitates, preserving the martensite structure and minimizing the loss of hardness and strength (45 steel reaches a hardness of HRC50-55 and a tensile strength of over 900 MPa after tempering). This is primarily used in applications requiring both high hardness and a certain degree of toughness (e.g., cutting tools and wear-resistant bushings).

Medium-temperature tempering (350-500°C): Martensite decomposes significantly into tempered troostite (fine-grained cementite + ferrite), reducing the hardness to 100%. At HRC 35-45, the strength remains at 700-800 MPa, while the elasticity is significantly improved (elastic limit reaches 300-400 MPa). It is suitable for springs and elastic components (such as automotive shock absorber springs and machine tool chucks).
High-temperature tempering (500-650°C): The martensite is completely decomposed into "tempered troostite" (coarse-grained cementite + ferrite), further reducing the hardness to HRC 25-35. The strength is maintained at 600-800 MPa, and the toughness and ductility are significantly improved. It is suitable for core parts requiring a balance of strength and toughness (such as shafts, connecting rods, and gears). 4. Stabilize microstructure and dimensions to ensure long-term part precision and reliability.
Quenched martensite is a non-equilibrium structure and still has a tendency to spontaneously decompose at room temperature (carbon slowly precipitates, gradually shifting the structure toward equilibrium). This "aging effect" can lead to the following during long-term use or storage:
Microstructural instability: Martensite slowly decomposes into pearlite or cementite, resulting in a gradual decline in properties (such as hardness and elasticity);
Dimensional instability: Microstructural transformation is accompanied by volume changes, leading to small but persistent deviations in part dimensions (e.g., dimensional accuracy loss in precision bearings and measuring tools).
Tempering accelerates martensite decomposition and carbide precipitation through "active heating," allowing the structure to reach a relatively stable state earlier (e.g., tempered bainite formed after high-temperature tempering undergoes almost no further microstructural transformation at room temperature). This results in:
Locking the microstructure: preventing performance fluctuations during subsequent use;
Fixing the dimensions: eliminating the risk of "aging deformation," ensuring the long-term dimensional accuracy of precision parts (such as machine tool spindles and precision bolts). 5. Facilitates Subsequent Processing (Improves Machinability)
The hardness of quenched steel is extremely high (e.g., 45 steel reaches HRC 55-60 after quenching). Direct cutting operations (such as turning and milling) face two major issues:
Rapid Tool Wear: High-hardness steel quickly wears high-speed steel or carbide cutting tools, resulting in high machining costs;
Low Machining Precision: Excessive hardness can easily lead to chipping and chatter marks during part cutting, making it difficult to maintain surface roughness (e.g., achieving an Ra value below 3.2μm).
Tempering the quenched steel at a medium-high temperature can reduce the hardness to HRC 25-40 (in the "easy-to-cut" range).
At this point, the steel's microstructure is tempered troostite or tempered troostite, resulting in moderate hardness. Tool forces are evenly distributed during cutting, resulting in slow wear.
The increased plasticity facilitates chip breakage (preventing tool wrapping), significantly improving surface finish quality (Ra values ​​can be reduced to below 1.6μm), paving the way for subsequent precision machining (e.g., finishing gears and shafts).