A36, A106 and GB Q195/Q235/Q355 Carbon Steel Coils: A Grade Guide for Hot-Rolled Black Coil

Sep 05, 2025 Leave a message

Why So Many Grade Names in One Enquiry

An enquiry listing A36, A106, Q195, Q235, Q355, Q345, S45 and DC01 in a single line reflects a buyer comparing carbon steels across standards and product forms. Each name carries a different guarantee: A36 (ASTM A36/A36M) is a structural carbon steel with a minimum yield of 250 MPa, supplied mainly as plate, flat bar and shapes; A106 (ASTM A106/A106M) is a seamless carbon steel pipe grade; Q195 and Q235 are general structural steels per GB/T 700; Q355 is a higher-strength structural steel per GB/T 1591; and DC01 is a cold-rolled low-carbon forming steel per EN 10130. Understanding what each designation guarantees prevents ordering the wrong product form for the job.

ASTM A36 and A106: The American References

A36 is the workhorse structural carbon steel of the Americas. For thickness up to 200 mm it guarantees minimum yield of 250 MPa (36 ksi) and tensile strength of 400-550 MPa, with carbon limited to 0.26% and welding-friendly characteristics. It is ordered as plate, coil for further processing, bars and shapes for buildings, bridges and machinery frames. A106 is a different product family: seamless carbon steel pipe for high-temperature service, with Grade B requiring minimum yield of 240 MPa and tensile of at least 415 MPa. The two names often appear together in an enquiry because a project needs both structural plate and pipe; they are not interchangeable product forms.

GB Q195, Q235 and Q355: The Chinese Structural Family

The Chinese designation starts with Q followed by the minimum yield strength in MPa. Q195 (GB/T 700) yields at least 195 MPa and is a soft, cheap grade for wire rod, light sections and simple stampings. Q235 (GB/T 700), the most widely used structural carbon steel in China, guarantees 235 MPa minimum yield with tensile of 370-500 MPa depending on thickness, and is used for buildings, bridges, vehicles and general fabrication. Q355 (GB/T 1591) guarantees 355 MPa minimum yield with better weldability and toughness than Q235, and is the standard choice for medium and heavy structures, cranes and mining equipment. Q345 is the former designation of this strength level, superseded by Q355 in GB/T 1591-2018; suppliers may still use the old name.

Grade Standard Min yield (MPa) Tensile Rm (MPa) Typical use
Q195 GB/T 700 195 315-430 Wire, light sections, stamping
Q235B GB/T 700 235 370-500 Structures, general fabrication
Q355B GB/T 1591 355 470-630 Heavy structures, cranes
A36 ASTM A36/A36M 250 400-550 Structural plate and shapes
A106 Gr B ASTM A106/A106M 240 415 min Seamless pipe, high-temp service

Hot-Rolled Black Coil vs Cold-Rolled DC01

Hot-rolled black coil is delivered with the dark mill scale surface left intact and is the economical base for thick, non-visible parts: structural sections, pipes, tanks, wheel rims and machine frames. The same chemistry can be cold rolled into DC01, which removes the scale by pickling, reduces the gauge and improves surface and tolerance for visible, formed parts. In procurement terms, a Q235 or A36 hot-rolled coil and a DC01 cold-rolled coil are different products for different operations; the choice follows the part thickness, the surface requirement and the forming severity, not just the chemistry.

Application Guidance

For building frames, purlins, fences and containers, Q235B or A36 hot-rolled coil and plate cover most needs at the lowest cost. Where load or span increases, move to Q355B for the strength-to-weight gain. For pipe lines and pressure service, order A106 seamless pipe with the required grade and wall thickness rather than coil. For deep-drawn or visible parts below about 3 mm, switch to cold-rolled DC grades per EN 10130. A practical check before ordering: confirm the product form (coil, plate, pipe), the thickness range, and which standard governs the destination market, then match the grade table above.

Quality Documents and Inspection

Request a mill certificate (EN 10204 Type 3.1 or the equivalent) showing the heat number, chemical composition and the yield and tensile test results for each lot. Check the certificate against the ordered grade, because Q235 and Q355 have different guaranteed values and substitution requires engineering approval. Inspect for laminations, edge cracks and heavy scale on hot-rolled surfaces, and confirm gauge with a micrometer at the strip edges and centre. Keep the certificate with the stock records so traceability survives to the fabrication shop.

Frequently Asked Questions

Is Q235 the same as A36? They are close but not identical. Q235 guarantees 235 MPa minimum yield per GB/T 700, while A36 guarantees 250 MPa per ASTM A36. Many buyers substitute them with engineering approval, but the standard, the certificate and the design code must be checked first.

What is the difference between Q355 and Q345? They are close but not identical. Q235 guarantees 235 MPa minimum yield per GB/T 700, while A36 guarantees 250 MPa per ASTM A36. Many buyers substitute them with engineering approval, but the standard, the certificate and the design code must be checked first.

is the former designation of 355 MPa yield structural steel, replaced by Q355 in GB/T 1591-2018 with adjusted composition and toughness requirements. New orders should be specified as Q355.? No. A106 is a specification for seamless carbon steel pipe, not for flat coil. For welded pipe from coil, specifications such as ASTM A53 or API 5L cover the appropriate material.

Can A106 pipe steel be supplied as coil? No. A106 is a specification for seamless carbon steel pipe, not for flat coil. For welded pipe from coil, specifications such as ASTM A53 or API 5L cover the appropriate material.

What does hot-rolled black coil mean? Black coil means hot-rolled strip delivered with the dark iron-oxide mill scale on the surface, without pickling or oiling. It is the standard economical form for structural and general engineering use before shot blasting or machining.

How do I choose between Q195 and Q235? Black coil means hot-rolled strip delivered with the dark iron-oxide mill scale on the surface, without pickling or oiling. It is the standard economical form for structural and general engineering use before shot blasting or machining.

is softer, cheaper and used for wire rod, light sections and simple stamping where 195 MPa yield is enough. Q235 is the general structural grade for load-carrying frames and parts; choose it whenever the component is stressed.? Both are low-carbon steels, but DC01 is a cold-rolled flat product with guaranteed forming properties per EN 10130, while Q195 is a general structural grade per GB/T 700 that may be supplied as hot-rolled product. They are not direct equivalents for forming applications.

Does DC01 belong to the same family as Q195? Both are low-carbon steels, but DC01 is a cold-rolled flat product with guaranteed forming properties per EN 10130, while Q195 is a general structural grade per GB/T 700 that may be supplied as hot-rolled product. They are not direct equivalents for forming applications.