A36 Q195 Q235 Q345b S235jr 3mm 10mm Thick Hot Cold Rolled Black Painted Galvanized Full Hard Mild Carbon Steel Plate A36

Jan 15, 2026 Leave a message

Overview of Common Structural Carbon Steel Grades

Structural carbon steel plates in thicknesses from 3 mm to 10 mm are produced in several widely used grades, including A36, Q195, Q235, Q345B and S235JR. Each grade is defined by a national or international standard: ASTM A36 for the American designation, GB/T 700 for Q195 and Q235, GB/T 1591 for Q345B, and EN 10025-2 for S235JR. Although these grades are sometimes treated as interchangeable in light fabrication, their specified yield strength, tensile range, toughness and weldability differ, and the correct choice depends on the load, the forming method and the service environment.

Grade Standard Min Yield (MPa) Tensile (MPa) Typical Use
Q195 GB/T 700 195 315-430 Light forming, wire, tubes
Q235 GB/T 700 235 370-500 General structures, frames
Q345B GB/T 1591 345 470-630 Heavier loaded structures
S235JR EN 10025-2 235 360-510 General construction
A36 ASTM A36 250 400-550 Bolted and welded structures

Mechanical Properties and Formability

For hot-rolled Q235 plate, the Brinell hardness typically falls in the range of 120-160 HBW, which gives a good balance between machinability and resistance to denting. All of these grades pass a 180° cold bend test in the thickness range mentioned above, meaning the plate can be folded flat on itself without cracking when the bend is made perpendicular to the rolling direction. The elongation after fracture is high enough for bending, rolling into cylinders and simple stamping operations.

Welding and Fabrication Guidance

Q235 and S235JR are low-carbon structural steels with excellent weldability. In normal shop conditions they can be welded without preheating using common filler metals such as the E43 series, which keeps fabrication cost low. Q345B needs slightly more care because of its higher manganese content and strength, and preheating may be required for thick sections or low ambient temperatures.

For simple stamping and bending, Q235 hot-rolled plate is adequate. If the component requires deep drawing or complex multi-stage forming, a cold-rolled drawing grade such as DC01 or DC06 to EN 10130 is a better choice, because the cold-rolled surface and controlled ductility reduce cracking and surface defects.

Heat Treatment Limitations

Q195 and Q235 are low-carbon steels, so they cannot be hardened by heat treatment. Quenching and tempering will not raise their strength because there is too little carbon to form a meaningful martensite structure. If higher strength is required, select a microalloyed grade such as Q345B or a quenched and tempered structural steel instead of trying to heat-treat a low-carbon grade.

Surface Conditions and Coating Options

These plates are available in several surface conditions: black (hot-rolled with mill scale), pickled, painted, or hot-dip galvanized. Black plate offers the lowest cost but rusts quickly outdoors; painted plate suits indoor or lightly exposed use; hot-dip galvanized plate to EN 10346 or GB/T 13912 provides long-term corrosion protection for outdoor structures, fences and frames.

FAQ

Q1. What is the difference between Q235 and S235JR?

Both have a minimum yield strength of 235 MPa. Q235 is defined by GB/T 700 with a tensile range of 370-500 MPa, while S235JR is defined by EN 10025-2 with a tensile range of 360-510 MPa and a guaranteed Charpy impact value of 27 J at 20°C.

Q2. Can Q235 plate be bent 180 degrees without cracking?

Yes. In the thickness range of 3-10 mm, Q235 passes the 180° cold bend test specified in GB/T 700, provided the bend axis is perpendicular to the rolling direction and the mandrel diameter follows the standard requirement.

Q3. Does Q235 need preheating before welding?

No. Q235 is a low-carbon steel and can normally be welded without preheating at ambient shop temperatures. For very thick sections or cold conditions, light preheating is still good practice.

Q4. Why is Q345B stronger than Q235?

Q345B is a low-alloy high-strength structural steel with a minimum yield of 345 MPa and a tensile strength of 470-630 MPa per GB/T 1591. The higher manganese and microalloy content provides strength through grain refinement and precipitation hardening.

Q5. Can I use Q235 for deep drawing?

Only for simple stamping. For deep drawing or complex forming, choose a cold-rolled drawing steel such as DC01 or DC06 to EN 10130, which offers better ductility and surface quality.

Q6. Can hot-rolled Q235 be hardened by heat treatment?

No. As a low-carbon steel it cannot be significantly hardened by quenching. If higher hardness or strength is required, select a different grade or apply surface treatments that suit low-carbon steel.