Alloy Steel with S50C Distributor Carbon Steel Sheet Pipe C10 C22 C45 C50 S10C S20C S45C 1010 1020 1045 1050 Steel Plate Flat BBlock Round Bar

May 12, 2026 Leave a message

What are the causes of peeling defects?

A: Inclusions in the cast billet, subcutaneous bubbles, and incomplete descaling during hot rolling; strictly control the purity of the cast billet and optimize hot rolling descaling.

What is the control range for surface roughness Ra?

A: Ordinary Ra 0.4-0.8μm, mirror finish Ra≤0.2μm; adjusted by roll roughness and rolling pressure.

What is the choice between oiled and oilless?

A: Oiling (rust-preventive oil/stamping oil) prevents rust and facilitates stamping; oilless is used for electroplating and requires degreasing before painting.

How is the formability of 1010 cold-rolled steel?

A: Excellent, elongation ≥35%, suitable for deep drawing, stretching, bending, and cold heading; can be made into complex shapes.

Minimum bending radius?

A: Soft state 0.5-1.0t (t = thickness), semi-hard state 1.0-2.0t, fully hard state 2.0-3.0t.