1.What are the main international and domestic standards systems?
International Standard: ISO
European Standard: EN
American Standard: ASTM
Chinese Standard: GB/T

2.What are the differences in chromium content requirements for chromate passivated surfaces?
Low chromium passivation: typically < 10 mg/m². It essentially does not alter the appearance of the galvanized sheet, maintaining its original metallic color. Primarily used for short-term rust prevention.
Lightweight passivation: 10 - 25 mg/m²
Medium-dose passivation 25 - 45 mg/m²

3.What are the different grades of chromium-free passivation?
Chromium-free passivation, light coating (L)
Chromium-free passivation, standard coating (M)
Chromium-free passivation, thick coating (H)

4.How to measure the passivation layer thickness/content?
X-ray fluorescence spectrometry (XRF):
This is the most commonly used and fastest non-destructive testing method. The instrument can directly measure the chromium (Cr) content (mg/m²) on the surface of galvanized coils.
This method requires calibration with standard samples but is ideal for rapid quality control on production lines.
Chemical titration:
This is a laboratory method. The chromium content in the solution is determined by dissolving the passivation film from a sample of known area and then titrating the solution.
The results are very accurate, but the process is complex and time-consuming, and is typically used for arbitration or precise analysis.
5.What are some things to keep in mind?
There are standards, but the focus is on "content" rather than "thickness": The standards primarily specify the chromium content in the passivation film using "milligrams per square meter (mg/m²)".
Grading System: Based on corrosion resistance requirements, it is divided into different grades such as L (light), M (medium), H (heavy), and S (extra heavy). The higher the grade, the higher the chromium content, the better the corrosion resistance, and the darker the color may be (especially yellow passivation).
Environmental Trends: Chromium-free passivation has become the mainstream, and its standards focus more on performance verification (such as salt spray test results) rather than specific chemical composition content.
Practical Application: When ordering galvanized coils, you need to clearly specify the passivation type and grade in the contract or technical agreement, for example: "Galvanized coil DX51D+Z, passivation treatment: chromium-free passivation, standard coating (M), salt spray test requirement ≥72 hours without white rust."