What Are DC01 to DC05 Cold Rolled Steel Grades?
Mechanical Property Ranges per EN 10130
EN 10130 specifies the following mechanical properties for thicknesses up to 3.0 mm (typical values quoted at 0.7 to 2.0 mm thickness):
| Grade | Yield strength Rp0.2 (MPa) | Tensile strength Rm (MPa) | Elongation A80 min (%) | Typical use |
|---|---|---|---|---|
| DC01 | 130-260 | 270-410 | 28 | Simple bending and forming |
| DC03 | 130-210 | 270-370 | 34 | Moderate forming |
| DC04 | 130-210 | 270-350 | 38 | Deep drawing |
| DC05 | 120-180 | 270-330 | 40 | Severe deep drawing |
Forming Behaviour and Surface Quality
As the grade number increases, the carbon content and yield strength decrease while elongation and strain-hardening capacity improve. DC04 and DC05 are supplied with guaranteed r90 (normal anisotropy) and n90 (strain hardening exponent) values when tested in accordance with EN 10130, which makes them predictable in multi-stage drawing operations. The surface of DC grades is produced to defined classes - DC01A (smooth), DC01B (bright) and DC01C (matte) - specified in EN 10130 for the different surface appearance requirements of painted or visible parts.
Grade Selection Guidance
Use DC01 for simple bending, beading, coining and shallow forming. Use DC03 where the part requires moderate stretching. Use DC04 for deep drawn parts such as automotive panels, housings and kitchenware. Use DC05 where the drawing ratio is high or where surface quality after forming is critical, such as exposed automotive body panels. Edge condition (untrimmed, trimmed, or slit edge) and dimensional tolerances should be agreed against EN 10131.
Frequently Asked Questions
Is DC01 stainless steel? No. DC01 is a cold-rolled low-carbon steel grade covered by EN 10130; it is not stainless steel. Stainless steels contain a minimum of about 10.5% chromium and are specified in standards such as EN 10088, which is a completely different material family.
What is the former designation of DC01? DC01 was previously designated St12 in DIN 1623 and FeP01 in older European nomenclature. The former designation of DC04 is St14.
Can DC01 be used for deep drawing? DC01 is suitable for simple forming operations such as bending and shallow drawing. For demanding deep drawing operations DC04 or DC05 should be selected because of their higher elongation and better anisotropy values.
What is the difference between DC03 and DC04? Both grades have similar yield and tensile strength ranges, but DC04 guarantees a higher minimum elongation (38% versus 34%) and better deep drawing parameters, so it is preferred for more severe deformation.
Is DC05 suitable for exposed automotive panels? Yes. DC05 combines low yield strength with high elongation and good surface quality classes, which is why it is widely specified for complex exterior body panels that are painted after forming.