DC01 SPCC St12 Cold Rolled Carbon Steel Coil

Dec 25, 2025 Leave a message

Q: Common problems and countermeasures during DC01 stamping?

A: Problems: Springback, cracking, surface scratches; Countermeasures: Optimize die clearance, control stamping speed, apply surface coating for protection.

Q: Key parameters for DC01 welding?

A: Use low-hydrogen electrodes for arc welding, with moderate current to prevent deformation; for resistance welding, strictly control pressure and energizing time to avoid incomplete welds.

Q: How to prevent rust on DC01?

A: Short-term use of rust-preventive paper/oil; long-term use can be electrophoresis, spraying, galvanizing/aluminized zinc plating, etc.

Q: Recommended bending radius for DC01?

A: Inner bending radius ≥ 0.5t (t is plate thickness) to avoid cracking.

Q: What is the purpose of annealing DC01?