Does the adhesion of the zinc coating on galvanized coils depend on humidity?

Nov 06, 2025 Leave a message

1.Why does humidity affect adhesion?

Surface Oxidation and Corrosion

During the galvanizing process, the surface of the steel strip immediately after exiting the zinc bath is pure and activated.

In a high-humidity environment, water molecules (H₂O) in the air are rapidly adsorbed onto the steel strip surface, reacting with zinc to form a loose, porous layer of basic zinc carbonate (commonly known as "white rust"), typically with the chemical formula Zn₅(CO₃)₂(OH)₆.

This white rust, unlike a dense alumina film, does not protect the internal metal. Its adhesion to the steel substrate is weak, and it hinders the subsequent formation of a strong Fe-Zn alloy layer (the core of the galvanized layer) between the molten zinc and the steel substrate.

Affecting the Formation of the Fe-Zn Alloy Layer

The bonding between the galvanized layer and the steel substrate relies on mutual diffusion at high temperatures to form a series of Fe-Zn alloy layers (Γ, δ, ζ phases).

If the steel substrate surface contains trace amounts of water film or corrosion products due to high humidity before entering the zinc bath, this metallurgical bonding process will be severely disrupted. This results in a discontinuous and uneven alloy layer, directly reducing adhesion.

Hydrogen accumulation (under specific conditions)

In the annealing furnace, rolling oil and moisture on the strip surface evaporate and decompose. If the ambient humidity is high, the strip surface may absorb even more moisture.

galvanized coil

2.What impact does it have on the production process?

Annealing Furnace Section: Excessive surface moisture in the strip before it enters the annealing furnace will affect the reduction effect and may introduce excessive hydrogen gas.

Air Knife Section and Cooling Tower Section: This is the critical area for zinc layer solidification and cooling. The extremely high humidity here will:

cause oxidation of the zinc layer surface before complete solidification, forming white rust.

rapid but uneven cooling may cause changes in internal stress within the zinc layer, affecting adhesion.

Passivation Process: If the passivated coating is not sufficiently dried in a high-humidity environment, residual moisture will be trapped under the film, potentially leading to underfilm corrosion and damaging the zinc layer over time.

galvanized coil

3.What are the impacts during storage and transportation?

Finished galvanized coils will condense when stored in a humid environment, especially when gaps between the coils create a capillary effect.

This condensation will continuously corrode the zinc layer, forming white rust. Severe white rust can make the zinc layer loose and easily scraped off, significantly reducing adhesion. This is the common "white rust" defect.

galvanized coil

4.How to deal with and control this?

Production workshop environmental control: Modern galvanizing production lines strictly control the temperature and humidity within the plant, especially in critical areas such as air knives and cooling towers.

Controlling the dew point of the protective gas: The dew point of the protective gas in the annealing furnace is an extremely important parameter. The lower the dew point, the drier the gas. By controlling the dew point, the reducing properties of the furnace atmosphere can be ensured, and moisture and hydrogen can be effectively removed.

Ensuring the passivation film is dry: After passivation, a thorough and uniform drying process is essential to ensure that the passivation film is completely cured and free of moisture.

 

5.How to standardize storage management?

Galvanized coils should be stored in an indoor warehouse, kept well-ventilated and dry.

Avoid direct contact with damp ground; use wooden supports to elevate them.

During humid seasons or in coastal areas, dehumidifiers or desiccants may be necessary.

When temporarily stored outdoors, they must be tightly covered with waterproof tarpaulins to prevent rain and moisture intrusion.