How to choose the right lubricant to protect the galvanized layer during stamping?

Sep 12, 2025 Leave a message

How to choose the right lubricant to protect the galvanized layer during stamping?

In the stamping process of SPCC-GI (hot-dip galvanized cold-rolled steel sheet), the lubricant must simultaneously meet three core requirements: reducing friction damage between the die and the coating, preventing chemical corrosion of the galvanized layer, and adapting to the strength of the stamping process. The specific selection principles and types are as follows:

1. Core Principles for Lubricant Selection

Chemical Compatibility:
The galvanized layer (zinc) is easily corroded by acidic and alkaline substances. Therefore, the lubricant must be neutral or slightly alkaline (pH 6.5-8.5). It must not contain strong acids (such as hydrochloric acid and sulfuric acid), strong bases (such as sodium hydroxide), or halogens (chlorine and fluorine) to prevent the coating from corroding, turning it white, and peeling. Lubrication Performance Matching:
Select lubrication intensity based on the complexity of the stamping process (shallow, deep, or drawing):
Shallow stamping/simple forming: Moderate lubricity is sufficient to avoid excessive lubricant residue that is difficult to clean.
Deep drawing/complex drawing: High extreme pressure resistance (containing extreme pressure additives such as sulfur, phosphorus, and zinc) is required to prevent intense friction between the die and the coating, which can lead to coating wear or high-temperature erosion.
Suitability for subsequent processes:
If welding or painting is required after stamping, the lubricant must:
Easy to remove before welding (no residue that affects conductivity);
Removable by cleaning agents before painting (no impact on coating adhesion).
Stability:
Resistant to delamination and deterioration over long-term use, and non-corrosive to the mold (avoiding rust caused by corrosive lubricants).