The surface quality of Q195 materials after cold processing (such as cold bending, stamping, cold rolling, and cold drawing) directly affects the product's appearance, corrosion resistance, and subsequent processing performance (such as painting and welding). Ensuring surface quality requires systematic control across three stages: pretreatment, process control, and post-processing. Specific measures are as follows:
1. Surface Pretreatment Before Processing: Eliminating Initial Defects
Q195 materials may have surface defects such as scale, rust, burrs, and oil stains before cold processing. These defects can be magnified during processing (for example, scale can be pressed into the surface, forming pits). Therefore, pretreatment is essential:
Rust and Scale Removal:
For materials with rust or scale, acid cleaning (with hydrochloric acid or sulfuric acid solutions), sandblasting, or shot blasting can be used to completely remove the surface oxide layer, exposing the clean metal substrate. After acid cleaning, rinse with clean water and neutralize the solution to prevent residual acid from corroding the surface.
Minor surface rust can also be removed by mechanical polishing (such as with sandpaper or a wire wheel) to ensure that there is no loose rust on the surface. Deburring and Smoothing:
Before cold working, inspect the material edges for burrs (such as the edges of sheared steel plates). Use a file, sanding belt, or specialized deburring equipment to prevent burrs from being pressed into the surface and causing scratches during stamping or cold bending.
Degreasing:
Oil contamination such as rolling oil and rust preventative oil on the material surface can impair lubrication (increasing localized friction). Before processing, wipe or clean the surface with a cleaning agent (such as kerosene or alkaline detergent) to ensure a clean surface.
II. Process Control: Reducing New Defects
During cold working, surface defects primarily arise from friction damage, stress concentration, and mold contamination. Targeted control measures are required:
Optimize mold design and condition:
Mold surface finish: Molds (such as stamping dies and cold rolling rollers) must be polished to Ra ≤ 0.8μm to prevent surface "copy" defects (i.e., transfer of mold roughness to the workpiece) caused by mold surface roughness (such as scratches and pits). Mold Material and Hardness: Use wear-resistant materials (such as Cr12 mold steel) and quench them to increase their hardness (HRC 58-62) to reduce contamination of the workpiece surface by debris generated by mold wear.
Avoid mold sticking/sticking: During cold drawing and cold rolling, iron filings or impurities in the mold can scratch the workpiece surface. During stamping, "sticking" (the material adhering to the mold) can cause surface tearing. Regular mold cleaning is necessary, and if necessary, chrome plating should be applied to the mold surface to enhance wear resistance and release properties.
Appropriate Lubricant Use:
Lubricants not only reduce friction but also form a protective film between the material and the mold, preventing "scratches" (such as streaking marks during cold rolling) caused by direct metal contact. Specific lubricants should be selected based on the processing method:
For stamping and cold bending: Use low-viscosity stamping oil (such as mineral oil with extreme pressure additives) for its good flowability, uniform surface coverage, and avoid localized lubrication deficiencies.
For cold drawing and cold rolling: Use high-viscosity grease or emulsion for its strong adhesion, ability to withstand high pressure, and prevent metal debris from embedding into the surface. Note: Lubricant must be clean and free of impurities. If it contains particles such as iron filings, it will "grind" the surface during processing, causing pitting or scratches.
Control processing parameters to avoid excessive deformation:
Excessive deformation or high speed during cold working can cause surface "wrinkling" (such as edge wrinkling during stamping and drawing) or "orange peel" (localized uneven plastic deformation). The deformation should be reasonably controlled (e.g., single-pass deformation rate ≤ 20% during drawing) and the processing speed should be maintained at a stable level (e.g., cold rolling speed should be controlled between 30-60 m/min).
During cold bending, the mold radius at the bend should be ≥ 1.5 times the material thickness to avoid surface cracking or microcracks caused by localized stress concentration. III. Post-Processing Surface Treatment: Repair and Protection
Even with rigorous machining controls, minor defects (such as fine scratches and residual lubricant) may still exist, requiring further optimization through post-processing:
Surface Cleaning:
Removing residual lubricant: Wipe the surface with a cleaning agent (such as gasoline or alcohol) to prevent residual lubricant from causing bubbles or cold welds during subsequent painting or welding.
Removing machining debris: Use compressed air or high-pressure water to remove metal powder adhering to the surface (especially after cold drawing and cold rolling) to prevent oxidation and rust from contaminating the surface.
Defect Repair:
Minor scratches or dents can be repaired through mechanical polishing (e.g., using a fine sanding belt or wool wheel) to restore the surface finish. Deeper defects (e.g., >0.1mm in depth) should be evaluated to determine if they will affect serviceability and, if necessary, scrapped.
Temporary Protection:
If subsequent treatment (such as painting) is not performed immediately after machining, the surface must be protected from rust. A thin layer of anti-rust oil can be sprayed on or covered with plastic wrap to prevent moisture and rust. Summary: Ensuring the surface quality of Q195 after cold working requires adhering to the principles of "prevention first, process control, and post-process repair": pre-treatment eliminates initial defects; during processing, optimizes molds, lubrication, and parameters to reduce new defects; and finally, improves the surface condition through cleaning and repair. For demanding applications (such as exterior parts), post-processing non-destructive testing (such as visual inspection and surface roughness measurement, Ra) is also necessary to ensure that surface quality meets standards (typically requiring Ra ≤ 3.2μm and the absence of defects such as cracks and rust).