What a PPGI Colour Coated Steel Coil Actually Is
PPGI stands for pre-painted galvanised iron. A PPGI colour coated steel coil is a cold rolled steel strip that first passes through a continuous hot dip galvanising line to receive a zinc or zinc alloy coating, and then through a coil coating line where a primer and a top coat are cured onto the surface. The finished coil combines the strength of cold reduced steel, the sacrificial corrosion protection of zinc and the decorative and protective behaviour of an organic paint film. Because the paint is applied in a continuous coil coating process rather than after fabrication, coating thickness, colour and gloss are far more uniform than with any brush or spray painting carried out on finished parts.
Cold Rolled Substrate Grades Used Under the Coating
The substrate decides formability, flatness and strength. Commercial quality cold reduced grades are the normal choice for roofing and cladding, while drawing grades are selected when the coated strip has to be profiled or bent to a tight radius. SPCC is the designation of a commercial quality cold rolled sheet produced under JIS G3141; it corresponds broadly to EN 10130 DC01 and to the older German grade ST12 of DIN 1623. SPCC is a plain carbon steel, not a stainless steel: it carries no deliberate chromium addition, so it cannot form the passive chromium oxide film that requires a minimum of 10.5% Cr.
| Substrate grade | Standard | Quality class | Typical role in PPGI |
|---|---|---|---|
| SPCC | JIS G3141 | Commercial | General roofing and wall cladding |
| DC01 | EN 10130 | Commercial | Panels, trim, general profiling |
| DC03 | EN 10130 | Drawing | Profiled sheet with tight bends |
| DC04 | EN 10130 | Deep drawing | Complex formed appliance parts |
| CS Type B | ASTM A1008 | Commercial | Metric-equivalent commercial sheet |
Selection follows the forming operation, not the decoration. A substrate with 140 to 280 MPa yield strength and at least 28% elongation in the commercial class handles ordinary roll forming without cracking, while drawing grades trade some strength for extra ductility.
Cold rolling at room temperature work hardens the steel. Compared with hot rolled strip of the same chemistry, the cold reduced product shows higher hardness, higher tensile strength, greater resistance to tension failure and greater resistance to deformation, and it offers a markedly smoother, oxide-free surface. That smooth surface matters for coil coating because paint adhesion, colour consistency and gloss all depend on a uniform substrate. Cold reduced strip also carries internal stress and lower elongation than fully annealed hot rolled material, so the annealing and skin pass schedule must be matched to the bending radius the customer intends to use.
Zinc Coating and Paint System Specifications
| Layer | Material | Typical range | Function |
|---|---|---|---|
| Zinc coating | Hot dip zinc per EN 10346 or ASTM A653 | Z100 to Z275, g/m2 total both sides | Sacrificial corrosion protection of cut edges |
| Pre-treatment | Chromate-free passivation or thin organic coating | Nanometre to 1 micron | Bonding and temporary transport protection |
| Primer | Epoxy or polyester primer | 4 to 6 micron | Adhesion and barrier layer |
| Top coat | Polyester, silicon modified polyester or PVDF | 18 to 25 micron | Colour, gloss and weather resistance |
| Back coat | Polyester or epoxy | 5 to 8 micron | Reverse side protection and marking |
Zinc coating mass and paint thickness must be quoted together. A heavier zinc coating improves edge and scratch protection but slightly reduces the bending performance of the strip, while a thicker paint film improves exterior durability but becomes more prone to cracking at very sharp radii.
Formability and Fabrication Notes
Roll forming: minimum bend radius normally 0.5 t to 1 t for commercial quality substrate at 0.4 to 0.8 mm gauge.
Cutting and punching: shearing exposes bare steel, so cut edges should be treated as a normal design allowance in corrosive atmospheres.
Fastening: self-drilling screws with sealing washers prevent water ingress at penetrations.
Stacking: store coils and sheets on dry, timber-supported racks to avoid white rust between contacting surfaces.
Welding: the organic coating must be stripped 10 to 20 mm each side of a weld and the joint repainted afterwards.
Typical Applications
Roof and wall cladding for factories, warehouses and cold storage buildings.
Corrugated and trapezoidal profiled sheet for agricultural and industrial construction.
Domestic appliance housings, refrigerator side panels and washing machine cabinets.
Doors, roller shutters, garage doors and ventilation ducting.
Containers, signage panels and general light-gauge fabrication.
Frequently Asked Questions
Q: Does cold rolled steel rust?
Yes. Cold rolled carbon steel has no alloy protection of its own, and exposed to moisture and air it gradually develops a rusted patina. That is exactly why a zinc coating plus a paint system is applied to the substrate in a PPGI coil.
Q: Why is cold rolled steel stronger than hot rolled steel?
Cold rolling deforms the metal at low temperature, and the resulting work hardening raises hardness, tensile strength, resistance to tension failure and resistance to deformation compared with hot rolled strip of the same analysis.
Q: Is SPCC stainless steel?
No. SPCC is a carbon steel grade of JIS G3141. It lacks the minimum 10.5% chromium needed to create the passive, corrosion-resistant surface layer that defines stainless steel.
Q: What is the difference between GI and PPGI coil?
GI is hot dip galvanised steel with a bare zinc surface. PPGI takes the same galvanised substrate and adds primer and top coat, giving colour, gloss and an extra barrier against weathering.
Q: Which paint system should be chosen for outdoor roofing?
Silicon modified polyester is the common choice for general exterior building panels; PVDF top coats are specified where long-term colour and gloss retention under strong ultraviolet exposure is the priority.
Q: How is zinc coating mass specified?
Zinc coating is quoted as total mass on both surfaces, for example Z275, which is a nominal 275 g/m2 total. The corresponding single-side average is used when corrosion life is calculated for a given environment.