How to handle excessive springback after bending SPCD rolls?
A: Increase the V-shaped opening width of the bending die to reduce local stress; use a bending die with a compensation angle; perform over-bending treatment on the material to offset the springback; alternatively, choose SPCD rolls that have undergone soft annealing to further reduce the probability of springback.
Can SPCD rolls be welded?
A: Yes. Their low carbon content is suitable for conventional welding methods such as spot welding and MIG/MAG welding. The joint strength after welding can match the base material, but parameters must be controlled during welding to avoid thermal deformation affecting accuracy.
How to solve the problem of severe deformation after welding SPCD rolls?
A: Optimize the welding sequence, use skip welding to disperse heat; use tooling fixtures to fix the workpiece and constrain deformation; use spot welding instead of continuous welding to reduce heat input; and perform timely straightening treatment after welding.
What are the causes of scratches on the surface of SPCD rolls?
A: 1. Contact with sharp objects during storage; 2. Rough or impurities on the die surface during processing; 3. Friction and collision between rolls during transportation. Proper packaging protection and die cleaning are necessary.
Does SPCD roll require surface pretreatment before processing?
Answer: Generally, simple pretreatment is required. If there is anti-rust oil on the surface, it needs to be wiped off or removed through a degreasing process before stamping to avoid affecting the lubrication effect. If there is slight oxidation on the surface, it can be treated by pickling or sandblasting to ensure processing quality.