What DC05 Material Stands For: EN 10130 Ultra-Deep Drawing Steel

Jun 04, 2025 Leave a message

DC05 is one of the highest formability grades in the European standard EN 10130, which covers cold rolled low carbon steel flat products for cold forming. The designation is built from three elements: D for deep drawing, C for cold rolled, and 05 as the performance level, where a higher number indicates better formability. Within EN 10130 the grade is intended for extremely complex stamping and ultra-deep drawing work, and it sits near the top of the conventional low carbon sequence, just below the interstitial-free grades.

Composition and Mechanical Requirements

DC05 is produced as an extra-low-carbon, fully killed steel with a tightly controlled grain structure. Carbon and other interstitial elements are held at very low levels so that the sheet retains the high plastic strain ratio and the high elongation that deep drawing demands. Table 1 lists the mechanical requirements of the EN 10130 grades.

Grade Yield strength Re max (MPa) Tensile strength Rm (MPa) Elongation A80 min (%)
DC01 280 270 to 410 28
DC03 240 270 to 370 34
DC04 210 270 to 350 38
DC05 180 270 to 330 40
DC06 170 270 to 330 41

Two consequences follow from the table. First, DC05 combines the lowest yield strength of the conventional part of the range with the highest elongation, which is exactly what an ultra-deep drawing operation needs: the material flows instead of tearing and springback stays low. Second, the permitted tensile range is narrow, from 270 to 330 MPa, so the grade is defined as much by consistency as by strength.

Published summaries sometimes quote an elongation of 38 percent for DC05. That figure belongs to DC04; EN 10130 requires at least 40 percent A80 for DC05.

DC05 Compared with SPCC and Other Cold Rolled Grades

SPCC is the general-purpose cold rolled carbon steel sheet and strip grade of JIS G3141, with a tensile strength commonly quoted between 270 and 410 MPa. It is specified for general structural parts and simple stampings that do not demand high formability, such as ordinary metal shells and straightforward brackets.

DC05 belongs to a different category of material. It is a European deep drawing grade with a guarantee of forming behaviour rather than a general-purpose commercial grade, and it is used in the automotive industry for body panels, fenders and hoods, and in electronics and appliances for housings and parts that must be stretched severely without failure. When translating a specification, the nearest Japanese equivalent is the drawing-quality SPCE of JIS G3141, and the nearest North American equivalent is the extra-deep drawing steel (EDDS) quality of ASTM A1008. The Chinese designation GB/T 5213 DC05 uses the same grade identifier as EN 10130.

Why DC05 Is Not Stainless Steel

DC05 is a plain cold rolled low carbon steel. It contains no chromium or nickel and therefore has no built-in corrosion resistance. In a humid or industrial atmosphere an unprotected DC05 part rusts quickly, and surface protection is mandatory rather than optional.

The usual answers are hot dip galvanizing, which produces the coated designation DC05+Z under EN 10346, electrolytic zinc coating for the equivalent DC05+ZE, or an organic paint system. Low carbon steel welds easily by resistance or arc processes, and the choice between them is normally driven by whether the sheet is supplied bare or coated, because a zinc coating changes the electrical and thermal behaviour of the joint.

Forming, Joining and Handling Notes

Drawing severity: DC05 can be stretched far beyond the capacity of DC01 or SPCC, but the tool has to be designed for it; insufficient blank holding force or a tight die radius will still tear the part.

Lubrication: high strain paths need a suitable drawing lubricant to keep friction low and prevent galling on the die.

Springback: the low yield strength keeps springback modest, which is an advantage for dimensional control of large panels.

Strain ageing and stretcher strains: skin-passed sheet should be used promptly, and stored coils of drawing quality sheet are normally consumed before ageing changes the surface appearance in forming.

Corrosion between operations: stamped parts should not be left unprotected in a humid workshop, because flash rust on the drawn surface will be visible after painting.

FAQ: DC05 Deep Drawing Steel

Q: What does DC05 stand for?
A: It is the EN 10130 designation for a cold rolled low carbon steel for deep drawing, where D means deep drawing, C means cold rolled and 05 is the formability level. A higher number indicates greater forming capability.

Q: What are the strength and elongation of DC05?
A: In EN 10130 the grade has a maximum yield strength of 180 MPa, a tensile strength range of 270 to 330 MPa and a minimum elongation A80 of 40 percent.

Q: Is DC05 stainless steel?
A: No. It is a low carbon steel without chromium or nickel, so it has no inherent corrosion resistance and must be galvanized, coated or painted for any exposed application.

Q: What is the difference between DC05 and SPCC?
A: SPCC is the JIS G3141 general-purpose cold rolled grade for ordinary stampings and structural parts, while DC05 is a European ultra-deep drawing grade with guaranteed formability. DC05 is used where the part cannot be produced from SPCC without cracking.

Q: Where is DC05 typically used?
A: Automotive body panels, fenders and hoods, fuel tanks, domestic appliance components and precision electronic housings, all of which require severe stretching with little or no load-bearing duty.

Q: Can DC05 be galvanized or welded?
A: Yes. Hot dip galvanized DC05+Z to EN 10346 and electrolytically coated DC05+ZE are standard products, and the low carbon content gives good weldability, although welding practice has to be adjusted when the sheet is zinc coated.

Q: Why is DC05 not used for structural parts?
A: Its strength is deliberately low so that it can be formed into complex shapes, which makes it unsuitable for load-bearing duty. Structural work calls for a grade such as EN 10025 S355J2 or GB/T 1591 Q355B instead.