What effect does the surface treatment process of galvanized coil have on its corrosion resistance?

Sep 16, 2025 Leave a message

1.What is the effect of passivation treatment on corrosion resistance?

Significantly reduces the formation of "white rust" (zinc oxide/zinc hydroxide) on the zinc layer: In humid environments, white rust may appear in 1-2 weeks on unpassivated galvanized coils, but this period can be extended to 1-3 months after passivation.
- Improves "self-healing after scratches": The passivation film can slightly repair minor scratches on the zinc layer, slowing localized corrosion at the scratched areas.
- Chromium-free passivation (environmentally friendly): While its corrosion protection is slightly lower than traditional chromate passivation (approximately 10%-20% lower), it complies with environmental standards such as RoHS and offers more stable long-term weathering performance.

galvanized sheet

2.What is the specific effect of oiling treatment on corrosion resistance?

Strong short-term corrosion protection: In short-term (3-6 months) humid environments such as storage and transportation, oiling completely prevents the formation of white rust, providing superior protection compared to simple passivation.
- Assists in repairing zinc coating defects: The oil film penetrates into the tiny pores of the zinc coating, filling defects and reducing corrosion penetration.

galvanized sheet

3.What is the specific impact of coating treatment on corrosion resistance?

Optimal long-term weather resistance: In outdoor exposure to sunlight and coastal high-salt fog environments, coating can increase the corrosion lifespan of galvanized coil by 2-3 times (for example, the lifespan of ordinary Z180 galvanized coil is 15 years, while coating can extend it to over 30 years).
Also, aesthetically pleasing: The coating can be customized in color and gloss, and it prevents scratches on the zinc layer during transportation.

galvanized sheet

4.What is the specific effect of phosphating treatment on corrosion resistance?

Enhanced "zinc layer + coating" synergistic protection: After coating un-phosphated galvanized coils, the coating is susceptible to peeling due to zinc corrosion. After phosphating, the phosphate film tightly bonds with the coating. Even if the coating is partially damaged, the phosphate film can slow the spread of corrosion, extending the overall corrosion protection life by 50%-100%.
- Improved salt spray resistance: The combination of phosphating and coating can increase the neutral salt spray resistance from 200 hours with coating alone to over 500 hours.

 

5.What is the key influence logic of surface treatment process on corrosion resistance?

Blocking the penetration of corrosive media
This is the core goal of all surface treatments. Passivation films, oil films, thin films, and phosphate films all form a "physical/chemical barrier" on the zinc surface, reducing the contact between water, oxygen, and chloride ions (chloride ions, a major corrosive agent in coastal environments) and the zinc layer. For example, the porosity of a chromium-free passivation film is only 1/10 that of a pure zinc layer, significantly reducing the penetration rate of corrosive media.
Inhibiting electrochemical corrosion of zinc
Zinc corrosion is essentially an electrochemical reaction in a "zinc-steel" galvanic cell (zinc acts as the anode, being consumed). Ingredients such as chromates and titanium salts used in passivation treatments form an "insulating layer" on the zinc surface, reducing the electrode activity of zinc and slowing the rate of electrochemical corrosion. The porous structure of the phosphate film also absorbs corrosion inhibitors, further inhibiting the reaction.
Repairing inherent defects in the zinc layer
The zinc layer of hot-dip galvanized coils inevitably contains defects such as tiny pores and scratches (excluding "missing plating spots"). These defects serve as "breakthrough points" for corrosion. The oil film of oil treatment can penetrate into the pores to fill defects; the passivation film can be formed preferentially at the defects to enhance local protection; the crystalline structure of the phosphate film can also cover tiny scratches to prevent defects from expanding.