Will the coating of color-coated steel rolls turn chalky after oxidation?

Dec 22, 2025 Leave a message

1.How does oxidation (degradation) lead to pulverization?

Oxidation/Degradation (Internal Chemical Changes):

The resin in the color-coated coil (such as polyester) undergoes complex chemical changes when exposed to the combined effects of ultraviolet (UV) radiation, heat, oxygen, and moisture outdoors for extended periods-a process known as "photo-oxidative degradation" or "thermal oxidative degradation."

This process disrupts the resin's molecular chains and chemical bonds, leading to a decrease in its degree of polymerization and a loose, brittle structure.

Loss of Adhesion (Critical Turning Point):

The resin acts as the "glue" in the coating, firmly binding pigment particles together and adhering them to the substrate.

As the resin degrades due to oxidation, its adhesive strength gradually weakens.

Chalking (External Physical Manifestation):

When the resin's adhesive strength weakens to the point where it can no longer encapsulate and fix the pigment particles, the outermost pigment particles begin to loosen and become exposed.

Under the influence of external forces such as wind, rain, and friction, these loose pigment particles detach from the coating surface, forming a layer of easily wiped-off powder. This is what we perceive as "chalking."

Color-coated rolls

2.What are the characteristics of the pulverization process?

Gradual Nature: Chalking is not sudden; it's a gradual process. Typically, loss of gloss and discoloration/yellowing occur first, followed by the chalking stage.

Starting from the Surface: Since ultraviolet (UV) energy is highest, degradation and chalking always begin at the outermost layer of the coating, gradually progressing to deeper layers.

Chalking Rate is Influenced by Several Factors:

Resin Type: Ordinary polyester (PE) is most prone to chalking; high-weather-resistant polyester (HDP) and silicone-modified polyester (SMP) have stronger resistance to chalking; PVDF (fluorocarbon) coatings exhibit the best resistance to chalking, maintaining their integrity even after decades of outdoor use.

Pigment Quality: Using high-quality, stable pigments (such as inorganic pigments and highly weather-resistant pigments) can delay chalking.

Environmental Conditions: Strong UV radiation, high temperature and humidity, and corrosive industrial or marine atmospheres accelerate the chalking process.

Coating Thickness: Sufficient coating thickness provides a longer degradation buffer period.

Color-coated rolls

3.What are the initial signs of coating chalking?

Loss of gloss, fading (color discoloration), yellowing: Oxidative degradation begins on the coating surface, and the structure of the surface resin and pigments changes.

Color-coated rolls

4.What are the characteristics of coating chalking in the middle stage?

It begins to powder; noticeable powder can be seen when rubbed with a finger or cloth.

The root cause is that the surface resin has degraded severely, lost its adhesive strength, and the pigment particles are exposed and begin to fall off.

 

5.What are the characteristics of coating chalking in the later stages?

Severe chalking, exposing the primer or substrate, may be accompanied by cracking and peeling.

The coating's protective function is essentially lost, allowing corrosive media (water, oxygen, ions) to directly attack the underlying metal.