1.What are the typical characteristics of waves on both sides? How to adjust them?
The edges of the strip are uneven.
• Adjust the rolls: Increase the roll crown appropriately.
• Adjust the bending rolls: Adjust the bending roll force; if necessary, switch to negative bending rolls.
• Optimize cooling: Ensure uniform cooling at both ends of the roll body; enhance cooling of the middle section.

2.What are the typical characteristics of a mid-wave pattern? How should it be adjusted?
The middle part of the strip is uneven
• Adjust the rolls: Use a reasonable (reduced) roll profile crown.
• Adjust the bending rolls: Appropriately reduce the positive bending roll force.
• Adjust the tension: Appropriately increase the front or back tension.

3.How to make good use of plate shape control?
Roll bending control: This is the most common and sensitive method. The roll gap shape is quickly changed by bending the work rolls using a hydraulic system. It's important to note that fluctuations in the bending force directly affect the strip shape; therefore, the hydraulic system must be kept stable.
Segmented cooling control: By spraying coolant in segments along the length of the roll, the thermal crown of the roll can be precisely controlled, thereby adjusting the local strip shape. For example, when double-sided waviness occurs, cooling of the middle section of the roll should be strengthened.
Tension control: Appropriately increasing tension helps to flatten the strip and suppress waviness. However, excessive tension can lead to narrowing or even breakage; therefore, it needs to be set carefully.

4.How to manage rolling mill rolls effectively?
Strictly control roll changing cycles: As rolling mileage increases, rolls wear down, and roll profile deteriorates. For extremely thin strip steel, roll changing cycles need to be shortened (e.g., reducing the steel throughput on the work rolls from 80t to below 60t).
Ensure roll preheating: Before rolling, the rolls must be fully preheated (e.g., for more than 25 minutes) to ensure uniform thermal expansion and prevent poor initial strip shape due to uneven temperature.
5.How to optimize process parameters?
Controlling rolling force: Excessive rolling force will exacerbate roll deflection and cause edge waviness. This can be addressed by optimizing the reduction per pass to distribute the load.
Pay attention to incoming material quality: The shape, thickness tolerance, and hardness uniformity of the incoming material directly affect the shape of the finished product. For severe incoming material waviness, adjustments need to be made in the preceding process (such as leveling).